PLASTIC FAMILY · ISO 1043: ABS

Acrylonitrile Butadiene Styrene (ABS)

ISO 1043: ABS · Styrenic Terpolymer · Amorphous · Variants: General Purpose, High-Impact ABS, Flame-Retardant (UL94 V-0), Electroplating Grade

Amorphous engineering-grade styrenic terpolymer combining impact toughness, dimensional stability, and surface finish quality for enclosures, housings, and electroplated parts.

Commodity Thermoplastic ABS ISO 1043: ABS Amorphous
Density
1.03 – 1.07 g/cm³
Tensile Strength
35 – 52 MPa
Flexural Modulus
1900 – 2600 MPa
Max Service Temp
70 – 85 °C
Glass Transition (Tg)
100 – 110 °C
PROPERTY BENCHMARKING

Key Mechanical & Thermal Comparison

ABS typical range Category range Database median
Density 1.03 – 1.07 g/cm³ (0.0372 – 0.0387 lb/in³)
0.85 g/cm³ Cat: 0.89 – 1.07 · Median: 1.05 1.3 g/cm³
Tensile Strength 35 – 52 MPa (5,080 – 7,540 psi)
15 MPa Cat: 20 – 52 · Median: 50 95 MPa
Flexural Modulus 1900 – 2600 MPa (276 – 377 ksi)
500 MPa Cat: 800 – 2600 · Median: 2200 3500 MPa
HDT @ 0.45 MPa 88 – 105 °C (190 – 221 °F)
50 °C Cat: 65 – 115 · Median: 105 240 °C
Max Continuous Service Temp 70 – 85 °C (158 – 185 °F)
50 °C Cat: 70 – 110 · Median: 100 150 °C

Source: ISO 1043 / MatWeb / Public Styrenic Resin Datasheets · Retrieved 2026-11-24 · Ranges represent unreinforced injection-molding grades unless noted

MATERIAL PROPERTIES

Typical Engineering Property Ranges

Acrylonitrile Butadiene Styrene property ranges
Property Typical Range (SI / Imperial)
Density 1.03 – 1.07 g/cm³ (0.0372 – 0.0387 lb/in³)
Tensile Strength (Yield / Break) 35 – 52 MPa (5,080 – 7,540 psi)
Flexural Modulus 1900 – 2600 MPa (276 – 377 ksi)
Elongation at Break 10 – 50 %
Notched Izod Impact (23 °C) 150 – 400 J/m (2.81 – 7.49 ft·lb/in)
HDT @ 0.45 MPa 88 – 105 °C (190 – 221 °F)
HDT @ 1.80 MPa 75 – 95 °C (167 – 203 °F)
Glass Transition (Tg) 100 – 110 °C (212 – 230 °F)
Max Continuous Service Temp 70 – 85 °C (158 – 185 °F)
Water Absorption (24 h, 23 °C) 0.2 – 0.4 %

Source: ISO 1043 / MatWeb / Public Styrenic Resin Datasheets · Retrieved 2026-11-24

MANUFACTURING & MOLDING

Processing Parameters

Acrylonitrile Butadiene Styrene processing parameters
Parameter Recommended Range
Melt Temperature 210 – 250 °C (410 – 482 °F)
Mold Temperature 40 – 80 °C (104 – 176 °F)
Drying Temperature 80 – 85 °C (176 – 185 °F)
Drying Time 2 – 4 h
Injection Pressure 70 – 130 MPa (10,150 – 18,850 psi)
Mold Shrinkage 0.4 – 0.7 %
Common Molding Processes Injection molding, Extrusion, Thermoforming, FDM 3D printing

Source: ISO 1043 / MatWeb / Public Styrenic Resin Datasheets · Retrieved 2026-11-24

APPLICATIONS & SELECTION

Typical Uses, Strengths & Limitations

Typical Industrial Applications
  • Electronic enclosures, instrumentation housings, and appliance panels
  • Automotive interior consoles and chrome-plated trim components
  • Protective equipment shells and consumer power-tool housings
  • Drain-waste-vent (DWV) piping and rigid extruded profiles
Key Advantages
  • Low, isotropic mold shrinkage (0.4 – 0.7%) for tight dimensional tolerances
  • Good impact strength and gloss surface aesthetics
  • Easily painted, adhesively bonded, ultrasonically welded, and electroplated
  • Broad processing window across standard injection presses
Design Limitations
  • Rapidly attacked by ketones (acetone), esters (ethyl acetate), and aromatics (toluene)
  • Poor outdoor weathering and UV stability due to butadiene phase
  • Moderate heat deflection ceiling compared with PC or PA66
  • Requires pre-drying before molding to prevent splay marks

Source: ISO 1043 / MatWeb / Public Styrenic Resin Datasheets · Retrieved 2026-11-24

CHEMICAL RESISTANCE

Common Chemicals vs. ABS

View full matrix →
ABS resistance to common chemicals
Chemical (CAS) Rating & Conditions Engineering Notes
Acetone
CAS 67-64-1 · C3H6O
D Not recommended 20 °C · 100% · Short-term contact Severe attack; acetone rapidly softens and dissolves the styrene-acrylonitrile phase of ABS.
Ethanol
CAS 64-17-5 · C2H6O
B Good 20 °C · 96 – 100% · Ambient contact Minor effect on unstressed ABS at 20 °C; high molded-in stress may promote slow environmental stress cracking.
Toluene
CAS 108-88-3 · C7H8
D Not recommended 20 °C · 100% · Short-term contact Severe attack; toluene rapidly dissolves and destroys ABS components.
Hydrochloric Acid (37%)
CAS 7647-01-0 · HCl
NR No data No verified test basis No data: published ratings for concentrated 37% HCl on ABS vary significantly by butadiene content and stabilizer grade; conduct immersion testing before use.
Sodium Hydroxide
CAS 1310-73-2 · NaOH
A Excellent 20 °C · 50% aqueous · Continuous immersion Good resistance to aqueous alkalis at ambient temperature; verify grades for elevated temperature CIP washdowns.
Ethyl Acetate
CAS 141-78-6 · C4H8O2
D Not recommended 20 °C · 100% · Short-term contact Severe attack; aliphatic esters rapidly soften and dissolve ABS.

Source: Cole-Parmer / Plastics Design Library · Retrieved 2026-11-24