CHEMICAL · CAS 100-42-5

Styrene

CAS 100-42-5 · EC 202-851-5 · C8H8 · UN2055

Reactive aromatic vinyl monomer that forms the backbone of polystyrene (GPPS/HIPS/EPS), ABS, SAN, SBR synthetic rubber, and unsaturated polyester fiberglass resins.

Also known as: Vinylbenzene, Phenylethylene, Ethenylbenzene, Styrene monomer (SM)

Molecular Weight
104.15 g/mol
Boiling Point
145.2 °C
Melting Point
-30.6 °C
Flash Point
31 °C
Density
0.9060 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Styrene chemical identifiers
Identifier Value
CAS Registry Number 100-42-5
EC Number 202-851-5
Molecular Formula C8H8
Molecular Weight 104.15 g/mol
IUPAC Name styrene
Canonical SMILES C=CC1=CC=CC=C1
InChI InChI=1S/C8H8/c1-2-8-6-4-3-5-7-8/h2-7H,1H2
InChIKey PPBRXRYQALVLMV-UHFFFAOYSA-N
UN Transport Number UN2055
PubChem CID 7501

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 7501

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Styrene (CAS 100-42-5) unless otherwise noted.

Density (vs. Water = 1.0)0.906 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-30.6 °C
-13020 °C260
Boiling Point145.2 °C
-50Water 100 °C350
Flash Point (Closed Cup)31 °C
-50GHS Cat.2 (23 °C)220
Styrene physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless to pale yellow oily liquid with sweet, penetrating aromatic odor
Density 0.9060 g/cm³ (20 °C) (7.56 lb/gal)
Melting Point -30.6 °C (-23.1 °F)
Boiling Point 145.2 °C (293.4 °F)
Flash Point 31 °C (87.8 °F (closed cup))
Vapor Pressure 6.4 mmHg (25 °C)
Water Solubility 0.31 g/L (25 °C)
pH / pKa Neutral aromatic monomer
Viscosity 0.696 mPa·s (25 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS02 Flammable
GHS08 Health Hazard
GHS07 Irritant / Harmful
Flammable Liquids (Category 3) · Acute Toxicity — Inhalation (Category 4) · Reproductive Toxicity (Category 2) · STOT — Repeated Exposure (Category 1, hearing organs)
Hazard statements
  • H226: Flammable liquid and vapor
  • H332: Harmful if inhaled
  • H361d: Suspected of damaging the unborn child
  • H372: Causes damage to hearing organs through prolonged inhalation
Key precautionary statements
  • P210: Keep away from heat, sparks, open flames and hot surfaces
  • P260: Do not breathe vapors
  • P280: Wear protective gloves, eye protection, and respirator where needed

Handling & storage: Store inhibited with 10–50 ppm TBC (4-tert-butylcatechol) below 25 °C to prevent runaway exothermic polymerization. Severely attacks PS, ABS, PC, PVC, PMMA; use PTFE, FEP, PEEK, PPS, or stainless steel.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Styrene

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Styrene
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to styrene monomer at 20 °C; moderate swelling, softening, or stress-cracking risk makes polypropylene (PP) unsuitable for continuous pressurized containment.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to styrene monomer at 20 °C; moderate swelling, softening, or stress-cracking risk makes HDPE unsuitable for continuous pressurized containment.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: styrene monomer causes severe chemical attack, dissolution, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: styrene monomer causes severe chemical attack, dissolution, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to styrene monomer at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA66 (Nylon 66).
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to styrene monomer at 20 °C; moderate swelling, softening, or stress-cracking risk makes LDPE unsuitable for continuous pressurized containment.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: styrene monomer causes severe chemical attack, dissolution, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: styrene monomer causes severe chemical attack, dissolution, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to styrene monomer at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA6 (Nylon 6).
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to styrene monomer at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to styrene monomer at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to styrene monomer at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: styrene monomer causes severe chemical attack, dissolution, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to styrene monomer at 20 °C; moderate swelling, softening, or stress-cracking risk makes UHMWPE unsuitable for continuous pressurized containment.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: styrene monomer causes severe chemical attack, dissolution, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to styrene monomer at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to styrene monomer at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PVDF.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to styrene monomer at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to styrene monomer at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to styrene monomer at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Styrene at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Styrene severely swells and degrades EPDM rubber; specify FKM (Viton) or PTFE/PFA seals for hydrocarbon or strong-acid service.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Styrene at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Styrene causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Styrene causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Catalytic dehydrogenation of ethylbenzene
  • Propylene oxide / styrene monomer (POSM) co-production
Downstream Derivatives
  • Polystyrene (GPPS, HIPS, EPS) and ABS/SAN engineering resins
  • Styrene-butadiene rubber (SBR) and latex
  • Reactive diluent in unsaturated polyester (FRP/fiberglass) resins
Typical Industrial Uses
  • Monomer for PS, ABS, SAN, and SBR tires/rubbers
  • Cross-linking reactive solvent for marine and industrial fiberglass composites
  • Ion-exchange resin bead synthesis

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Styrene & Compatible Equipment

Styrene Industrial / Reagent Grade (CAS 100-42-5)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Styrene Bulk Chemical Suppliers & Packaging

Verified ISO-certified chemical manufacturers

View Suppliers on Made-in-China.com