PLASTIC FAMILY · ISO 1629: NBR

Nitrile Butadiene Rubber (Buna-N) (NBR)

ISO 1629: NBR · Elastomer · Amorphous · Variants: Standard ACN (33%), High-ACN (40–45%, Oil Resistant), HNBR (Hydrogenated), Carboxylated XNBR

Workhorse oil- and fuel-resistant synthetic rubber offering high abrasion resistance and low cost for hydraulic seals, fuel hoses, aliphatic hydrocarbon gaskets, and general industrial O-rings.

Industrial Elastomer NBR ISO 1629: NBR Amorphous
Density
1.15 – 1.3 g/cm³
Tensile Strength
12 – 22 MPa
Flexural Modulus
6 – 28 MPa
Max Service Temp
95 – 110 °C
Glass Transition (Tg)
-40 – -25 °C
PROPERTY BENCHMARKING

Key Mechanical & Thermal Comparison

NBR typical range Category range Database median
Density 1.15 – 1.3 g/cm³ (0.0415 – 0.0470 lb/in³)
0.85 g/cm³ Cat: 1.05 – 1.95 · Median: 1.2 2.25 g/cm³
Tensile Strength 12 – 22 MPa (1,740 – 3,190 psi)
5 MPa Cat: 6 – 22 · Median: 46 115 MPa
Flexural Modulus 6 – 28 MPa (0.9 – 4.1 ksi)
0 MPa Cat: 3 – 30 · Median: 2250 4400 MPa
Max Continuous Service Temp 95 – 110 °C (203 – 230 °F)
50 °C Cat: 95 – 210 · Median: 100 270 °C

Source: ISO 1629 / Parker O-Ring Handbook / Public Elastomer Datasheets · Retrieved 2026-11-25 · Ranges represent unreinforced injection-molding grades unless noted

MATERIAL PROPERTIES

Typical Engineering Property Ranges

Nitrile Butadiene Rubber (Buna-N) property ranges
Property Typical Range (SI / Imperial)
Density 1.15 – 1.3 g/cm³ (0.0415 – 0.0470 lb/in³)
Tensile Strength (Yield / Break) 12 – 22 MPa (1,740 – 3,190 psi)
Flexural Modulus 6 – 28 MPa (0.9 – 4.1 ksi)
Elongation at Break 200 – 500 %
Notched Izod Impact (23 °C) —
HDT @ 0.45 MPa —
HDT @ 1.80 MPa —
Glass Transition (Tg) -40 – -25 °C (-40 – -13 °F)
Max Continuous Service Temp 95 – 110 °C (203 – 230 °F)
Water Absorption (24 h, 23 °C) 0.3 – 1.2 %

Source: ISO 1629 / Parker O-Ring Handbook / Public Elastomer Datasheets · Retrieved 2026-11-25

MANUFACTURING & MOLDING

Processing Parameters

Nitrile Butadiene Rubber (Buna-N) processing parameters
Parameter Recommended Range
Melt Temperature 155 – 185 °C (311 – 365 °F)
Mold Temperature 155 – 180 °C (311 – 356 °F)
Drying Temperature —
Drying Time —
Injection Pressure 50 – 110 MPa (7,250 – 15,950 psi)
Mold Shrinkage 1.5 – 2.5 %
Common Molding Processes Compression molding, Rubber injection molding, Hose extrusion, Dipping (gloves)

Source: ISO 1629 / Parker O-Ring Handbook / Public Elastomer Datasheets · Retrieved 2026-11-25

APPLICATIONS & SELECTION

Typical Uses, Strengths & Limitations

Typical Industrial Applications
  • Hydraulic cylinder seals, rotary shaft oil seals, and pneumatic O-rings
  • Petroleum fuel transfer hoses, diesel gaskets, and lubricant filters
  • Chemical-resistant disposable and industrial protective gloves
  • Industrial rollers and abrasion-resistant pump stators
Key Advantages
  • Excellent resistance to mineral oils, hydraulic fluids, greases, and aliphatic hydrocarbons (hexane/heptane)
  • Good mechanical strength, tear resistance, and abrasion resistance
  • Economical cost and broad availability across Shore A 40–90 hardnesses
Design Limitations
  • Poor resistance to ozone, outdoor UV weathering, and high heat (>105 °C; use HNBR or FKM)
  • Attacked by ketones, esters, chlorinated hydrocarbons, aromatic solvents, and strong oxidizing acids

Source: ISO 1629 / Parker O-Ring Handbook / Public Elastomer Datasheets · Retrieved 2026-11-25

CHEMICAL RESISTANCE

Common Chemicals vs. NBR

View full matrix →
NBR resistance to common chemicals
Chemical (CAS) Rating & Conditions Engineering Notes
Acetone
CAS 67-64-1 · C3H6O
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Acetone causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Ethanol
CAS 64-17-5 · C2H6O
B Good 20 °C · 96 – 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Ethanol at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Toluene
CAS 108-88-3 · C7H8
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Toluene causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Hydrochloric Acid (37%)
CAS 7647-01-0 · HCl
C Fair 20 °C · 37% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Hydrochloric Acid (37%) at 20 °C; moderate swelling, softening, or stress-cracking risk makes NBR (Buna-N) nitrile rubber unsuitable for continuous containment.
Sodium Hydroxide
CAS 1310-73-2 · NaOH
B Good 20 °C · 40 – 50% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Sodium Hydroxide at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Ethyl Acetate
CAS 141-78-6 · C4H8O2
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Ethyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Methanol
CAS 67-56-1 · CH4O
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Methanol at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Isopropanol (IPA)
CAS 67-63-0 · C3H8O
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Isopropanol (IPA) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Ethylene Glycol
CAS 107-21-1 · C2H6O2
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Ethylene Glycol at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
1-Butanol
CAS 71-36-3 · C4H10O
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to 1-Butanol at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Methyl Ethyl Ketone (MEK)
CAS 78-93-3 · C4H8O
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Methyl Ethyl Ketone (MEK) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Tetrahydrofuran (THF)
CAS 109-99-9 · C4H8O
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Tetrahydrofuran (THF) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
n-Butyl Acetate
CAS 123-86-4 · C6H12O2
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
n-Hexane
CAS 110-54-3 · C6H14
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-Hexane at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Cyclohexane
CAS 110-82-7 · C6H12
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Cyclohexane at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Styrene
CAS 100-42-5 · C8H8
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Styrene causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Dichloromethane (DCM)
CAS 75-09-2 · CH2Cl2
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Dichloromethane (DCM) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Chloroform
CAS 67-66-3 · CHCl3
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Chloroform causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
N,N-Dimethylformamide (DMF)
CAS 68-12-2 · C3H7NO
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N,N-Dimethylformamide (DMF) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Dimethyl Sulfoxide (DMSO)
CAS 67-68-5 · C2H6OS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Dimethyl Sulfoxide (DMSO) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
N-Methyl-2-pyrrolidone (NMP)
CAS 872-50-4 · C5H9NO
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N-Methyl-2-pyrrolidone (NMP) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Sulfuric Acid (98%)
CAS 7664-93-9 · H2O4S
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Sulfuric Acid (98%) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Nitric Acid (65%)
CAS 7697-37-2 · HNO3
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Nitric Acid (65%) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Phosphoric Acid (85%)
CAS 7664-38-2 · H3O4P
B Good 20 °C · 85% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Phosphoric Acid (85%) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Hydrogen Peroxide (30%)
CAS 7722-84-1 · H2O2
D Not recommended 20 °C · 30% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Hydrogen Peroxide (30%) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Sodium Hypochlorite (12.5%)
CAS 7681-52-9 · ClNaO
D Not recommended 20 °C · 12.5% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Sodium Hypochlorite (12.5%) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Acetic Acid (Glacial)
CAS 64-19-7 · C2H4O2
D Not recommended 20 °C · 100% (Glacial) · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Acetic Acid (Glacial) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Formic Acid (85%)
CAS 64-18-6 · CH2O2
D Not recommended 20 °C · 85% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Formic Acid (85%) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Potassium Hydroxide (KOH)
CAS 1310-58-3 · HKO
B Good 20 °C · 45 – 50% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Potassium Hydroxide (KOH) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Ammonium Hydroxide (25%)
CAS 1336-21-6 · H5NO
B Good 20 °C · 25% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Ammonium Hydroxide (25%) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Methyl Isobutyl Ketone (MIBK)
CAS 108-10-1 · C6H12O
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Methyl Isobutyl Ketone (MIBK) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Cyclohexanone
CAS 108-94-1 · C6H10O
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Cyclohexanone causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Methyl Acetate
CAS 79-20-9 · C3H6O2
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Methyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Isopropyl Acetate
CAS 108-21-4 · C5H10O2
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Isopropyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
PGMEA (PMA)
CAS 108-65-6 · C6H12O3
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: PGMEA (PMA) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Diethyl Ether
CAS 60-29-7 · C4H10O
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Diethyl Ether causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Methyl tert-Butyl Ether (MTBE)
CAS 1634-04-4 · C5H12O
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Methyl tert-Butyl Ether (MTBE) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
1,4-Dioxane
CAS 123-91-1 · C4H8O2
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 1,4-Dioxane causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Benzene
CAS 71-43-2 · C6H6
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Benzene causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Ethylbenzene
CAS 100-41-4 · C8H10
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Ethylbenzene causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
p-Xylene
CAS 106-42-3 · C8H10
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: p-Xylene causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
n-Heptane
CAS 142-82-5 · C7H16
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-Heptane at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
n-Pentane
CAS 109-66-0 · C5H12
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-Pentane at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Trichloroethylene (TCE)
CAS 79-01-6 · C2HCl3
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Tetrachloroethylene (PCE)
CAS 127-18-4 · C2Cl4
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Tetrachloroethylene (PCE) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Acetonitrile
CAS 75-05-8 · C2H3N
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Acetonitrile causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Propylene Glycol (PG)
CAS 57-55-6 · C3H8O2
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Propylene Glycol (PG) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Glycerol (Glycerin)
CAS 56-81-5 · C3H8O3
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Glycerol (Glycerin) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Diethylene Glycol (DEG)
CAS 111-46-6 · C4H10O3
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Diethylene Glycol (DEG) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
2-Butoxyethanol
CAS 111-76-2 · C6H14O2
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 2-Butoxyethanol causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Benzyl Alcohol
CAS 100-51-6 · C7H8O
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Benzyl Alcohol causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Isobutanol
CAS 78-83-1 · C4H10O
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Isobutanol at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
1-Propanol
CAS 71-23-8 · C3H8O
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to 1-Propanol at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Phenol
CAS 108-95-2 · C6H6O
D Not recommended 20 °C · 90 – 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Bisphenol A (BPA)
CAS 80-05-7 · C15H16O2
A Excellent 20 °C · Solid / Aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Bisphenol A (BPA) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Methyl Methacrylate (MMA)
CAS 80-62-6 · C5H8O2
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Methyl Methacrylate (MMA) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Acrylic Acid
CAS 79-10-7 · C3H4O2
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Acrylic Acid causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
n-Butyl Acrylate
CAS 141-32-2 · C7H12O2
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acrylate causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Vinyl Acetate Monomer (VAM)
CAS 108-05-4 · C4H6O2
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Vinyl Acetate Monomer (VAM) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Acrylonitrile
CAS 107-13-1 · C3H3N
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Acrylonitrile causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Caprolactam
CAS 105-60-2 · C6H11NO
B Good 20 °C · Solid / Aq. · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Caprolactam at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Adipic Acid
CAS 124-04-9 · C6H10O4
B Good 20 °C · Solid / Aq. · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Adipic Acid at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Terephthalic Acid (PTA)
CAS 100-21-0 · C8H6O4
A Excellent 20 °C · Solid · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Terephthalic Acid (PTA) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Phthalic Anhydride
CAS 85-44-9 · C8H4O3
B Good 20 °C · Solid · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Phthalic Anhydride at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Maleic Anhydride
CAS 108-31-6 · C4H2O3
D Not recommended 20 °C · Solid / Aq. · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Maleic Anhydride causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Epichlorohydrin (ECH)
CAS 106-89-8 · C3H5ClO
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Dioctyl Phthalate (DOP / DEHP)
CAS 117-81-7 · C24H38O4
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Dioctyl Phthalate (DOP / DEHP) at 20 °C; moderate swelling, softening, or stress-cracking risk makes NBR (Buna-N) nitrile rubber unsuitable for continuous containment.
Dioctyl Terephthalate (DOTP)
CAS 6422-86-2 · C24H38O4
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Dioctyl Terephthalate (DOTP) at 20 °C; moderate swelling, softening, or stress-cracking risk makes NBR (Buna-N) nitrile rubber unsuitable for continuous containment.
Dibutyl Phthalate (DBP)
CAS 84-74-2 · C16H22O4
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Dibutyl Phthalate (DBP) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Dioctyl Adipate (DOA)
CAS 103-23-1 · C22H42O4
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Dioctyl Adipate (DOA) at 20 °C; moderate swelling, softening, or stress-cracking risk makes NBR (Buna-N) nitrile rubber unsuitable for continuous containment.
Acetyl Tributyl Citrate (ATBC)
CAS 77-90-7 · C20H34O8
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Acetyl Tributyl Citrate (ATBC) at 20 °C; moderate swelling, softening, or stress-cracking risk makes NBR (Buna-N) nitrile rubber unsuitable for continuous containment.
Citric Acid
CAS 77-92-9 · C6H8O7
A Excellent 20 °C · 10 – 50% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Citric Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Oxalic Acid
CAS 144-62-7 · C2H2O4
B Good 20 °C · 10% aq. · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Oxalic Acid at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Lactic Acid
CAS 50-21-5 · C3H6O3
B Good 20 °C · 85% aq. · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Lactic Acid at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Benzoic Acid
CAS 65-85-0 · C7H6O2
B Good 20 °C · Solid / Sat. aq. · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Benzoic Acid at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Formaldehyde (37% Formalin)
CAS 50-00-0 · CH2O
B Good 20 °C · 37% aq. · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Formaldehyde (37% Formalin) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Glutaraldehyde (50%)
CAS 111-30-8 · C5H8O2
B Good 20 °C · 50% aq. · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Glutaraldehyde (50%) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
N,N-Dimethylacetamide (DMAc)
CAS 127-19-5 · C4H9NO
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N,N-Dimethylacetamide (DMAc) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Monoethanolamine (MEA)
CAS 141-43-5 · C2H7NO
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Monoethanolamine (MEA) at 20 °C; moderate swelling, softening, or stress-cracking risk makes NBR (Buna-N) nitrile rubber unsuitable for continuous containment.
Triethanolamine (TEA)
CAS 102-71-6 · C6H15NO3
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethanolamine (TEA) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Triethylamine (Et3N)
CAS 121-44-8 · C6H15N
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Triethylamine (Et3N) at 20 °C; moderate swelling, softening, or stress-cracking risk makes NBR (Buna-N) nitrile rubber unsuitable for continuous containment.
Aniline
CAS 62-53-3 · C6H7N
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Ethylenediamine (EDA)
CAS 107-15-3 · C2H8N2
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Ethylenediamine (EDA) at 20 °C; moderate swelling, softening, or stress-cracking risk makes NBR (Buna-N) nitrile rubber unsuitable for continuous containment.
Urea
CAS 57-13-6 · CH4N2O
A Excellent 20 °C · 32.5% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Urea at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Hydrofluoric Acid (48% HF)
CAS 7664-39-3 · FH
D Not recommended 20 °C · 48% aq. · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Hydrofluoric Acid (48% HF) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Perchloric Acid (70%)
CAS 7601-90-3 · ClHO4
D Not recommended 20 °C · 70% aq. · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Boric Acid
CAS 10043-35-3 · BH3O3
A Excellent 20 °C · Sat. aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Boric Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Sodium Carbonate (Soda Ash)
CAS 497-19-8 · CNa2O3
A Excellent 20 °C · 20% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Sodium Carbonate (Soda Ash) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Sodium Bicarbonate
CAS 144-55-8 · CHNaO3
A Excellent 20 °C · Sat. aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Sodium Bicarbonate at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Sodium Chloride (Brine)
CAS 7647-14-5 · ClNa
A Excellent 20 °C · 26% brine · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Sodium Chloride (Brine) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Sodium Sulfate
CAS 7757-82-6 · Na2O4S
A Excellent 20 °C · Sat. aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Sodium Sulfate at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Calcium Chloride
CAS 10043-52-4 · CaCl2
A Excellent 20 °C · 35% brine · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Calcium Chloride at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Ferric Chloride (40% Solution)
CAS 7705-08-0 · Cl3Fe
A Excellent 20 °C · 40% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Ferric Chloride (40% Solution) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Copper(II) Sulfate
CAS 7758-98-7 · CuO4S
A Excellent 20 °C · Sat. aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Copper(II) Sulfate at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Potassium Permanganate
CAS 7722-64-7 · KMnO4
D Not recommended 20 °C · 10% aq. · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Potassium Permanganate causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Calcium Hydroxide (Hydrated Lime)
CAS 1305-62-0 · CaH2O2
A Excellent 20 °C · Slurry · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Calcium Hydroxide (Hydrated Lime) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Sodium Lauryl Sulfate (SLS)
CAS 151-21-3 · C12H25NaO4S
A Excellent 20 °C · 30% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Sodium Lauryl Sulfate (SLS) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Titanium Dioxide (TiO2)
CAS 13463-67-7 · O2Ti
A Excellent 20 °C · Solid · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Titanium Dioxide (TiO2) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Silicon Dioxide (Fumed Silica)
CAS 7631-86-9 · O2Si
A Excellent 20 °C · Solid · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Silicon Dioxide (Fumed Silica) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
1,4-Butanediol (BDO)
CAS 110-63-4 · C4H10O2
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to 1,4-Butanediol (BDO) at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.

Source: Parker O-Ring Handbook / Cole-Parmer Elastomer Compatibility Consensus · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source NBR by Grade & Form Factor

NBR O-Rings & Flange Gaskets

Standard ACN (33%) · Chemical sealing grades

View Suppliers on Made-in-China.com
NBR Rubber Sheets, Hoses & Custom Molded Seals

Extruded tubing, sheets & custom rubber molding

View Suppliers on Made-in-China.com