CHEMICAL · CAS 102-71-6

Triethanolamine (TEA)

CAS 102-71-6 · EC 203-049-8 · C6H15NO3

High-boiling tertiary alkanolamine widely used as a cement grinding aid, CNC metalworking fluid corrosion inhibitor, and mild pH neutralizer in detergents and cosmetics.

Also known as: 2,2',2''-Nitrilotriethanol, Trolamine, TEA

Molecular Weight
149.19 g/mol
Boiling Point
335.4 °C
Melting Point
21.6 °C
Flash Point
179 °C
Density
1.124 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Triethanolamine (TEA) chemical identifiers
Identifier Value
CAS Registry Number 102-71-6
EC Number 203-049-8
Molecular Formula C6H15NO3
Molecular Weight 149.19 g/mol
IUPAC Name 2-[bis(2-hydroxyethyl)amino]ethanol
Canonical SMILES C(CO)N(CCO)CCO
InChI InChI=1S/C6H15NO3/c8-4-1-7(2-5-9)3-6-10/h8-10H,1-6H2
InChIKey GSEJCLTVZPLZKY-UHFFFAOYSA-N
UN Transport Number —
PubChem CID 7618

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 7618

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Triethanolamine (TEA) (CAS 102-71-6) unless otherwise noted.

Density (vs. Water = 1.0)1.124 g/cm³
0.5Water 1.02.5
Melting / Freezing Point21.6 °C
-13020 °C260
Boiling Point335.4 °C
-50Water 100 °C350
Flash Point (Closed Cup)179 °C
-50GHS Cat.2 (23 °C)220
Triethanolamine (TEA) physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless to pale yellow viscous hygroscopic liquid with faint amine odor
Density 1.124 g/cm³ (20 °C) (9.38 lb/gal)
Melting Point 21.6 °C (70.9 °F)
Boiling Point 335.4 °C (635.7 °F)
Flash Point 179 °C (354.2 °F (closed cup))
Vapor Pressure <0.001 mmHg (25 °C)
Water Solubility Miscible in all proportions
pH / pKa pH 10.5 (1% aq.); pKa 7.76
Viscosity 609 mPa·s (25 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Warning
GHS07 Irritant / Harmful
Skin Irritation (Cat. 2) · Serious Eye Irritation (Cat. 2A)
Hazard statements
  • H315: Causes skin irritation
  • H319: Causes serious eye irritation
Key precautionary statements
  • P264: Wash thoroughly after handling
  • P280: Wear protective gloves and eye protection

Handling & storage: Store above 25 °C in sealed HDPE, PP, or stainless steel drums away from acids/nitrites. Compatible with PP, HDPE, PTFE, FEP, PFA, PEEK, PPS, and EPDM; avoid PC and PET.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Triethanolamine (TEA)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Triethanolamine (TEA)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in polypropylene (PP).
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in HDPE.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in ABS.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethanolamine (TEA) causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in PA66 (Nylon 66).
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in LDPE.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethanolamine (TEA) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethanolamine (TEA) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in PA6 (Nylon 6).
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in acetal (POM).
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethanolamine (TEA) causes severe attack, swelling, crazing, or rapid structural failure in PBT even under short-term contact.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethanolamine (TEA) causes severe attack, swelling, crazing, or rapid structural failure in PET even under short-term contact.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethanolamine (TEA) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in UHMWPE.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in SAN.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Triethanolamine (TEA) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in PVDF.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Triethanolamine (TEA) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Triethanolamine (TEA) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethanolamine (TEA) at 20 °C with negligible swelling, weight change, or mechanical degradation in EPDM rubber.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethanolamine (TEA) causes rapid swelling, softening, and seal failure in FKM (Viton) fluoroelastomer; consider EPDM or PTFE/FEP-encapsulated seals instead.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethanolamine (TEA) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethanolamine (TEA) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Reaction of three equivalents of ethylene oxide with ammonia
Downstream Derivatives
  • Portland cement grinding aids and concrete early-strength admixtures
  • Metalworking fluid corrosion inhibitors and cosmetic/detergent emulsifiers
Typical Industrial Uses
  • Global standard grinding aid and strength enhancer in cement production
  • pH buffer and corrosion inhibitor in CNC metalworking coolants
  • Emulsifier and surfactant neutralizer in detergents and personal care

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Triethanolamine (TEA) & Compatible Equipment

Triethanolamine Industrial / Reagent Grade (CAS 102-71-6)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Triethanolamine Bulk Chemical Suppliers & Packaging

Verified ISO-certified chemical manufacturers

View Suppliers on Made-in-China.com