p-Xylene
High-volume aromatic isomer separated from mixed xylenes, serving as the primary global feedstock for purified terephthalic acid (PTA) and PET polyester.
Also known as: para-Xylene, 1,4-Dimethylbenzene, PX
Registry Numbers & Structural Strings
| Identifier | Value |
|---|---|
| CAS Registry Number | 106-42-3 |
| EC Number | 203-396-5 |
| Molecular Formula | C8H10 |
| Molecular Weight | 106.16 g/mol |
| IUPAC Name | 1,4-xylene |
| Canonical SMILES | CC1=CC=C(C=C1)C |
| InChI | InChI=1S/C8H10/c1-7-3-5-8(2)6-4-7/h3-6H,1-2H3 |
| InChIKey | URLKBWYHVLBVBO-UHFFFAOYSA-N |
| UN Transport Number | UN1307 |
| PubChem CID | 7809 |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 7809
Measured Constants (SI / Imperial)
Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous p-Xylene (CAS 106-42-3) unless otherwise noted.
| Property | Value |
|---|---|
| Physical State | Liquid |
| Appearance | Colorless liquid with sweet aromatic odor (freezes at 13.3 °C) |
| Density | 0.861 g/cm³ (20 °C) (7.18 lb/gal) |
| Melting Point | 13.3 °C (55.9 °F) |
| Boiling Point | 138.4 °C (281.1 °F) |
| Flash Point | 27 °C (80.6 °F (closed cup)) |
| Vapor Pressure | 8.84 mmHg (25 °C) |
| Water Solubility | 0.162 g/L (25 °C) |
| pH / pKa | Non-polar aromatic |
| Viscosity | 0.603 mPa·s (25 °C) |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
GHS Classification & Precautions
- H226: Flammable liquid and vapor
- H304: May be fatal if swallowed and enters airways
- H312+H332: Harmful in contact with skin or inhaled
- P210: Keep away from heat, sparks, and open flames
- P280: Wear chemical gloves and eye protection
Handling & storage: Keep above 15 °C in traced lines to prevent crystallization. Attacks ABS, PC, PS, PMMA, PVC-U, EPDM, and NBR; specify PTFE, FEP, PFA, PVDF, PEEK, PPS, or FKM.
Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25
Plastics in Contact with p-Xylene
Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.
| Plastic Family | Rating & Conditions | Engineering Notes |
|---|---|---|
| Polypropylene (PP)
ISO 1043: PP | Limited resistance to p-Xylene at 20 °C; moderate swelling, softening, or stress-cracking risk makes polypropylene (PP) unsuitable for continuous containment. Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C) | |
| High-Density Polyethylene (HDPE)
ISO 1043: PE-HD | Limited resistance to p-Xylene at 20 °C; moderate swelling, softening, or stress-cracking risk makes HDPE unsuitable for continuous containment. Grade basis: High-density polyethylene (PE100 / blow-molding HDPE) | |
| Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS | Not recommended: p-Xylene causes severe attack, swelling, crazing, or rapid structural failure in ABS even under short-term contact. Grade basis: General-purpose unreinforced ABS molding grade | |
| Polycarbonate (PC)
ISO 1043: PC | Not recommended: p-Xylene causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact. Grade basis: Unfilled bisphenol-A polycarbonate (PC) | |
| Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66 | Excellent resistance to p-Xylene at 20 °C with negligible swelling, weight change, or mechanical degradation in PA66 (Nylon 66). Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66) | |
| Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD | Limited resistance to p-Xylene at 20 °C; moderate swelling, softening, or stress-cracking risk makes LDPE unsuitable for continuous containment. Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade) | |
| Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U | Not recommended: p-Xylene causes severe attack, swelling, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact. Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade) | |
| Polystyrene (GPPS) (PS)
ISO 1043: PS | Not recommended: p-Xylene causes severe attack, swelling, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact. Grade basis: General-purpose crystal polystyrene (GPPS) | |
| Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6 | Excellent resistance to p-Xylene at 20 °C with negligible swelling, weight change, or mechanical degradation in PA6 (Nylon 6). Grade basis: Unreinforced polyamide 6 (extruded/molded PA6) | |
| Polyoxymethylene (Acetal) (POM)
ISO 1043: POM | Excellent resistance to p-Xylene at 20 °C with negligible swelling, weight change, or mechanical degradation in acetal (POM). Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H) | |
| Polybutylene Terephthalate (PBT)
ISO 1043: PBT | Excellent resistance to p-Xylene at 20 °C with negligible swelling, weight change, or mechanical degradation in PBT. Grade basis: Unreinforced polybutylene terephthalate (PBT) | |
| Polyethylene Terephthalate (PET)
ISO 1043: PET | Good resistance to p-Xylene at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Semi-crystalline / oriented PET resin | |
| Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA | Not recommended: p-Xylene causes severe attack, swelling, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact. Grade basis: Cast & extruded polymethyl methacrylate (PMMA) | |
| Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW | Limited resistance to p-Xylene at 20 °C; moderate swelling, softening, or stress-cracking risk makes UHMWPE unsuitable for continuous containment. Grade basis: Virgin compression-molded UHMWPE (>3M g/mol) | |
| Styrene-Acrylonitrile (SAN)
ISO 1043: SAN | Not recommended: p-Xylene causes severe attack, swelling, crazing, or rapid structural failure in SAN even under short-term contact. Grade basis: Transparent styrene-acrylonitrile copolymer (SAN) | |
| Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE | Virtually inert to p-Xylene at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade) | |
| Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF | Excellent resistance to p-Xylene at 20 °C with negligible swelling, weight change, or mechanical degradation in PVDF. Grade basis: Homopolymer PVDF (pipe, valve & sheet grade) | |
| Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP | Good resistance to p-Xylene at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Melt-extruded FEP tubing & lining grade | |
| Polyether Ether Ketone (PEEK)
ISO 1043: PEEK | Excellent resistance to p-Xylene at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK. Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class) | |
| Polyphenylene Sulfide (PPS)
ISO 1043: PPS | Excellent resistance to p-Xylene at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS. Grade basis: Linear / 40% glass-filled PPS (PPS-GF40) | |
| Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA | Virtually inert to p-Xylene at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: High-purity melt-processable PFA tubing & lining grade | |
| Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM | Not recommended: p-Xylene severely swells and degrades EPDM rubber; specify FKM (Viton) or PTFE/PFA seals for hydrocarbon or strong-acid service. Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A) | |
| Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM | Excellent resistance to p-Xylene at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer. Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine) | |
| Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR | Not recommended: p-Xylene causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact. Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N) | |
| Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ | Not recommended: p-Xylene causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact. Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ) |
Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25
Upstream, Downstream & Applications
- Catalytic reforming of naphtha followed by simulated moving-bed (Parex) separation and xylene isomerization
- Purified terephthalic acid (PTA) and dimethyl terephthalate (DMT) for PET bottles and polyester fibers
- Parylene conformal coating dimers
- Global petrochemical feedstock for PTA and PET polyester resins/fibers
- Specialty aromatic solvent and parylene electronics coating precursor
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
Source p-Xylene & Compatible Equipment
High-purity industrial grade · Bulk supply
View Suppliers on Made-in-China.comHDPE / PTFE / FKM / EPDM solvent transfer equipment