CHEMICAL · CAS 106-89-8

Epichlorohydrin (ECH)

CAS 106-89-8 · EC 203-439-8 · C3H5ClO · UN2023

Bifunctional chlorinated epoxide monomer reacted with Bisphenol A to produce the vast majority of global epoxy resins for composites, electronics, and coatings.

Also known as: 2-(Chloromethyl)oxirane, 1-Chloro-2,3-epoxypropane, ECH

Molecular Weight
92.52 g/mol
Boiling Point
116.5 °C
Melting Point
-57.2 °C
Flash Point
31 °C
Density
1.181 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Epichlorohydrin (ECH) chemical identifiers
Identifier Value
CAS Registry Number 106-89-8
EC Number 203-439-8
Molecular Formula C3H5ClO
Molecular Weight 92.52 g/mol
IUPAC Name 2-(chloromethyl)oxirane
Canonical SMILES C1C(O1)CCl
InChI InChI=1S/C3H5ClO/c4-1-3-2-5-3/h3H,1-2H2
InChIKey BRLQWZUYTZBJKN-UHFFFAOYSA-N
UN Transport Number UN2023
PubChem CID 7835

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 7835

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Epichlorohydrin (ECH) (CAS 106-89-8) unless otherwise noted.

Density (vs. Water = 1.0)1.181 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-57.2 °C
-13020 °C260
Boiling Point116.5 °C
-50Water 100 °C350
Flash Point (Closed Cup)31 °C
-50GHS Cat.2 (23 °C)220
Epichlorohydrin (ECH) physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless mobile liquid with pungent chloroform-like odor
Density 1.181 g/cm³ (20 °C) (9.86 lb/gal)
Melting Point -57.2 °C (-71 °F)
Boiling Point 116.5 °C (241.7 °F)
Flash Point 31 °C (87.8 °F (closed cup))
Vapor Pressure 16.5 mmHg (25 °C)
Water Solubility 65.9 g/L (20 °C)
pH / pKa Neutral reactive epoxide
Viscosity 1.12 mPa·s (20 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS02 Flammable
GHS05 Corrosive
GHS06 Acute Toxicity
GHS08 Health Hazard
Flammable Liquids (Cat. 3) · Acute Toxicity — Oral/Dermal/Inhalation (Cat. 3) · Skin Corrosion (Cat. 1B) · Carcinogenicity (Cat. 1B)
Hazard statements
  • H226: Flammable liquid and vapor
  • H301+H311+H331: Toxic if swallowed, in contact with skin or inhaled
  • H314: Causes severe skin burns
  • H350: May cause cancer
Key precautionary statements
  • P201: Obtain special instructions before use
  • P210: Keep away from ignition sources
  • P280: Wear full chemical PPE and respiratory protection

Handling & storage: Store cool and dry away from acids, bases, and amines (violent ring-opening polymerization). Restrict wetted materials to PTFE, FEP, PFA, PEEK, PPS, or stainless steel.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Epichlorohydrin (ECH)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Epichlorohydrin (ECH)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Epichlorohydrin (ECH) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Epichlorohydrin (ECH) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in PA66 (Nylon 66) even under short-term contact.
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in LDPE even under short-term contact.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in PA6 (Nylon 6) even under short-term contact.
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Epichlorohydrin (ECH) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Epichlorohydrin (ECH) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PBT unsuitable for continuous containment.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Epichlorohydrin (ECH) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PET unsuitable for continuous containment.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Epichlorohydrin (ECH) at 20 °C; moderate swelling, softening, or stress-cracking risk makes UHMWPE unsuitable for continuous containment.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Epichlorohydrin (ECH) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Epichlorohydrin (ECH) at 20 °C with negligible swelling, weight change, or mechanical degradation in PVDF.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Epichlorohydrin (ECH) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Epichlorohydrin (ECH) at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Epichlorohydrin (ECH) at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Epichlorohydrin (ECH) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Epichlorohydrin (ECH) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes rapid swelling, softening, and seal failure in FKM (Viton) fluoroelastomer; consider EPDM or PTFE/FEP-encapsulated seals instead.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Epichlorohydrin (ECH) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Chlorination of propylene via allyl chloride
  • Bio-based glycerol-to-epichlorohydrin (GTE) process
Downstream Derivatives
  • Liquid and solid epoxy resins (reaction with Bisphenol A)
  • Paper wet-strength resins (PAE) and epichlorohydrin elastomers (ECO)
Typical Industrial Uses
  • Essential co-monomer for DGEBA epoxy adhesives, composites, and PCB laminates
  • Feedstock for wet-strength paper additives and water-treatment polyamines
  • Monomer for fuel-resistant ECO synthetic rubber

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Epichlorohydrin (ECH) & Compatible Equipment

Epichlorohydrin Industrial / Reagent Grade (CAS 106-89-8)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Epichlorohydrin Bulk Chemical Suppliers & Packaging

Verified ISO-certified chemical manufacturers

View Suppliers on Made-in-China.com