Acrylonitrile
Critical petrochemical nitrile monomer produced by propylene ammoxidation, supplying ABS/SAN plastics, NBR oil-resistant rubber, and carbon-fiber PAN precursors.
Also known as: Prop-2-enenitrile, Vinyl cyanide, AN
Registry Numbers & Structural Strings
| Identifier | Value |
|---|---|
| CAS Registry Number | 107-13-1 |
| EC Number | 203-466-5 |
| Molecular Formula | C3H3N |
| Molecular Weight | 53.06 g/mol |
| IUPAC Name | prop-2-enenitrile |
| Canonical SMILES | C=CC#N |
| InChI | InChI=1S/C3H3N/c1-2-3-4/h2H,1H2 |
| InChIKey | NLHHRLWOUZZQLW-UHFFFAOYSA-N |
| UN Transport Number | UN1093 |
| PubChem CID | 7855 |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 7855
Measured Constants (SI / Imperial)
Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Acrylonitrile (CAS 107-13-1) unless otherwise noted.
| Property | Value |
|---|---|
| Physical State | Liquid |
| Appearance | Colorless volatile liquid with pungent onion-garlic odor |
| Density | 0.806 g/cm³ (20 °C) (6.73 lb/gal) |
| Melting Point | -83.5 °C (-118.3 °F) |
| Boiling Point | 77.3 °C (171.1 °F) |
| Flash Point | 0 °C (32 °F (closed cup)) |
| Vapor Pressure | 109 mmHg (25 °C) |
| Water Solubility | 73.5 g/L (20 °C) |
| pH / pKa | Neutral nitrile monomer |
| Viscosity | 0.34 mPa·s (25 °C) |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
GHS Classification & Precautions
- H225: Highly flammable liquid and vapor
- H301+H311+H331: Toxic if swallowed, in contact with skin or inhaled
- H318: Causes serious eye damage
- H350: May cause cancer
- P201: Obtain special instructions before use
- P210: Keep away from ignition sources
- P280: Use closed transfer systems and full toxic-vapor PPE
Handling & storage: Store inhibited (MEHQ) strictly away from strong bases/amines (triggers violent exothermic polymerization). Restrict wetted polymers to PTFE, FEP, PFA, PEEK, or PPS.
Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25
Plastics in Contact with Acrylonitrile
Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.
| Plastic Family | Rating & Conditions | Engineering Notes |
|---|---|---|
| Polypropylene (PP)
ISO 1043: PP | Good resistance to Acrylonitrile at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C) | |
| High-Density Polyethylene (HDPE)
ISO 1043: PE-HD | Good resistance to Acrylonitrile at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: High-density polyethylene (PE100 / blow-molding HDPE) | |
| Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS | Not recommended: Acrylonitrile causes severe attack, swelling, crazing, or rapid structural failure in ABS even under short-term contact. Grade basis: General-purpose unreinforced ABS molding grade | |
| Polycarbonate (PC)
ISO 1043: PC | Not recommended: Acrylonitrile causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact. Grade basis: Unfilled bisphenol-A polycarbonate (PC) | |
| Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66 | Excellent resistance to Acrylonitrile at 20 °C with negligible swelling, weight change, or mechanical degradation in PA66 (Nylon 66). Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66) | |
| Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD | Good resistance to Acrylonitrile at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade) | |
| Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U | Not recommended: Acrylonitrile causes severe attack, swelling, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact. Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade) | |
| Polystyrene (GPPS) (PS)
ISO 1043: PS | Not recommended: Acrylonitrile causes severe attack, swelling, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact. Grade basis: General-purpose crystal polystyrene (GPPS) | |
| Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6 | Excellent resistance to Acrylonitrile at 20 °C with negligible swelling, weight change, or mechanical degradation in PA6 (Nylon 6). Grade basis: Unreinforced polyamide 6 (extruded/molded PA6) | |
| Polyoxymethylene (Acetal) (POM)
ISO 1043: POM | Good resistance to Acrylonitrile at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H) | |
| Polybutylene Terephthalate (PBT)
ISO 1043: PBT | Limited resistance to Acrylonitrile at 20 °C; moderate swelling, softening, or stress-cracking risk makes PBT unsuitable for continuous containment. Grade basis: Unreinforced polybutylene terephthalate (PBT) | |
| Polyethylene Terephthalate (PET)
ISO 1043: PET | Limited resistance to Acrylonitrile at 20 °C; moderate swelling, softening, or stress-cracking risk makes PET unsuitable for continuous containment. Grade basis: Semi-crystalline / oriented PET resin | |
| Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA | Not recommended: Acrylonitrile causes severe attack, swelling, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact. Grade basis: Cast & extruded polymethyl methacrylate (PMMA) | |
| Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW | Good resistance to Acrylonitrile at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Virgin compression-molded UHMWPE (>3M g/mol) | |
| Styrene-Acrylonitrile (SAN)
ISO 1043: SAN | Not recommended: Acrylonitrile causes severe attack, swelling, crazing, or rapid structural failure in SAN even under short-term contact. Grade basis: Transparent styrene-acrylonitrile copolymer (SAN) | |
| Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE | Virtually inert to Acrylonitrile at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade) | |
| Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF | Good resistance to Acrylonitrile at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Homopolymer PVDF (pipe, valve & sheet grade) | |
| Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP | Virtually inert to Acrylonitrile at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: Melt-extruded FEP tubing & lining grade | |
| Polyether Ether Ketone (PEEK)
ISO 1043: PEEK | Excellent resistance to Acrylonitrile at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK. Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class) | |
| Polyphenylene Sulfide (PPS)
ISO 1043: PPS | Excellent resistance to Acrylonitrile at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS. Grade basis: Linear / 40% glass-filled PPS (PPS-GF40) | |
| Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA | Virtually inert to Acrylonitrile at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: High-purity melt-processable PFA tubing & lining grade | |
| Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM | Limited resistance to Acrylonitrile at 20 °C; moderate swelling, softening, or stress-cracking risk makes EPDM rubber unsuitable for continuous containment. Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A) | |
| Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM | Not recommended: Acrylonitrile causes rapid swelling, softening, and seal failure in FKM (Viton) fluoroelastomer; consider EPDM or PTFE/FEP-encapsulated seals instead. Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine) | |
| Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR | Not recommended: Acrylonitrile causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact. Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N) | |
| Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ | Not recommended: Acrylonitrile causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact. Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ) |
Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25
Upstream, Downstream & Applications
- Sohio catalytic ammoxidation of propylene with ammonia and air
- ABS and SAN engineering thermoplastics
- Polyacrylonitrile (PAN) acrylic fibers and carbon-fiber precursors
- NBR nitrile rubber and acrylamide water-treatment polymers
- Key comonomer providing chemical/heat resistance in ABS, SAN, and NBR rubber
- Primary precursor for aerospace/industrial carbon fibers (PAN)
- Feedstock for adiponitrile (PA66) and polyacrylamide flocculants
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
Source Acrylonitrile & Compatible Equipment
High-purity industrial grade · Bulk supply
View Suppliers on Made-in-China.comVerified ISO-certified chemical manufacturers
View Suppliers on Made-in-China.com