CHEMICAL · CAS 108-05-4

Vinyl Acetate Monomer (VAM)

CAS 108-05-4 · EC 203-545-4 · C4H6O2 · UN1301

Major vinyl ester monomer essential for EVA solar-panel encapsulants, PVAc adhesives/paints, polyvinyl alcohol (PVOH), and EVOH barrier packaging.

Also known as: Ethenyl acetate, VAM

Molecular Weight
86.09 g/mol
Boiling Point
72.7 °C
Melting Point
-93.2 °C
Flash Point
-8 °C
Density
0.932 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Vinyl Acetate Monomer (VAM) chemical identifiers
Identifier Value
CAS Registry Number 108-05-4
EC Number 203-545-4
Molecular Formula C4H6O2
Molecular Weight 86.09 g/mol
IUPAC Name ethenyl acetate
Canonical SMILES CC(=O)OC=C
InChI InChI=1S/C4H6O2/c1-3-6-4(2)5/h3H,1H2,2H3
InChIKey XTXRWKRVRITETP-UHFFFAOYSA-N
UN Transport Number UN1301
PubChem CID 7904

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 7904

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Vinyl Acetate Monomer (VAM) (CAS 108-05-4) unless otherwise noted.

Density (vs. Water = 1.0)0.932 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-93.2 °C
-13020 °C260
Boiling Point72.7 °C
-50Water 100 °C350
Flash Point (Closed Cup)-8 °C
-50GHS Cat.2 (23 °C)220
Vinyl Acetate Monomer (VAM) physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless volatile liquid with sweet-pungent ethereal odor
Density 0.932 g/cm³ (20 °C) (7.78 lb/gal)
Melting Point -93.2 °C (-135.8 °F)
Boiling Point 72.7 °C (162.9 °F)
Flash Point -8 °C (17.6 °F (closed cup))
Vapor Pressure 115 mmHg (25 °C)
Water Solubility 20 g/L (20 °C)
pH / pKa Neutral vinyl ester
Viscosity 0.43 mPa·s (20 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS02 Flammable
GHS06 Acute Toxicity
GHS08 Health Hazard
GHS07 Irritant / Harmful
Flammable Liquids (Cat. 2) · Acute Toxicity — Inhalation (Cat. 4) · Carcinogenicity (Cat. 2) · STOT — Single Exposure (Cat. 3)
Hazard statements
  • H225: Highly flammable liquid and vapor
  • H332: Harmful if inhaled
  • H335: May cause respiratory irritation
  • H351: Suspected of causing cancer
Key precautionary statements
  • P210: Keep away from heat, sparks, and open flames
  • P280: Wear protective gloves and eye protection

Handling & storage: Store inhibited (hydroquinone) in cool, grounded tanks away from acids/bases (hydrolyzes to acetaldehyde/acetic acid). Use PTFE, FEP, PFA, PEEK, or PPS; avoid ABS, PC, PVC-U, PS, PMMA.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Vinyl Acetate Monomer (VAM)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Vinyl Acetate Monomer (VAM)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Vinyl Acetate Monomer (VAM) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Vinyl Acetate Monomer (VAM) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Vinyl Acetate Monomer (VAM) causes severe attack, swelling, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Vinyl Acetate Monomer (VAM) causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Vinyl Acetate Monomer (VAM) at 20 °C with negligible swelling, weight change, or mechanical degradation in PA66 (Nylon 66).
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Vinyl Acetate Monomer (VAM) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Vinyl Acetate Monomer (VAM) causes severe attack, swelling, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Vinyl Acetate Monomer (VAM) causes severe attack, swelling, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Vinyl Acetate Monomer (VAM) at 20 °C with negligible swelling, weight change, or mechanical degradation in PA6 (Nylon 6).
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Vinyl Acetate Monomer (VAM) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Vinyl Acetate Monomer (VAM) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Vinyl Acetate Monomer (VAM) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Vinyl Acetate Monomer (VAM) causes severe attack, swelling, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Vinyl Acetate Monomer (VAM) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Vinyl Acetate Monomer (VAM) causes severe attack, swelling, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Vinyl Acetate Monomer (VAM) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Vinyl Acetate Monomer (VAM) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Vinyl Acetate Monomer (VAM) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Vinyl Acetate Monomer (VAM) at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Vinyl Acetate Monomer (VAM) at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Vinyl Acetate Monomer (VAM) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Vinyl Acetate Monomer (VAM) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Vinyl Acetate Monomer (VAM) causes rapid swelling, softening, and seal failure in FKM (Viton) fluoroelastomer; consider EPDM or PTFE/FEP-encapsulated seals instead.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Vinyl Acetate Monomer (VAM) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Vinyl Acetate Monomer (VAM) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Vapor-phase acetoxylation of ethylene with acetic acid and oxygen over Pd catalyst
Downstream Derivatives
  • Polyvinyl acetate (PVAc) wood glues and emulsion paints
  • Polyvinyl alcohol (PVOH) and Ethylene-Vinyl Acetate (EVA) solar encapsulants
  • EVOH barrier packaging films
Typical Industrial Uses
  • Monomer for EVA photovoltaic solar encapsulation films and footwear foams
  • Feedstock for PVAc white wood adhesives and architectural latex paints
  • Precursor for PVOH water-soluble films and EVOH oxygen-barrier packaging

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Vinyl Acetate Monomer (VAM) & Compatible Equipment

Vinyl Acetate Monomer Industrial / Reagent Grade (CAS 108-05-4)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Vinyl Acetate Monomer Bulk Chemical Suppliers & Packaging