Isopropyl Acetate
Medium-fast evaporating ester solvent prized in flexible-packaging printing inks, coatings, and pharmaceutical extraction for its balanced drying rate.
Also known as: Propan-2-yl acetate, IPAC
Registry Numbers & Structural Strings
| Identifier | Value |
|---|---|
| CAS Registry Number | 108-21-4 |
| EC Number | 203-561-1 |
| Molecular Formula | C5H10O2 |
| Molecular Weight | 102.13 g/mol |
| IUPAC Name | propan-2-yl acetate |
| Canonical SMILES | CC(C)OC(=O)C |
| InChI | InChI=1S/C5H10O2/c1-4(2)7-5(3)6/h4H,1-3H3 |
| InChIKey | JMMWKPVZQRWMSS-UHFFFAOYSA-N |
| UN Transport Number | UN1220 |
| PubChem CID | 7915 |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 7915
Measured Constants (SI / Imperial)
Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Isopropyl Acetate (CAS 108-21-4) unless otherwise noted.
| Property | Value |
|---|---|
| Physical State | Liquid |
| Appearance | Clear, colorless liquid with mild fruity odor |
| Density | 0.872 g/cm³ (20 °C) (7.28 lb/gal) |
| Melting Point | -73.4 °C (-100.1 °F) |
| Boiling Point | 88.6 °C (191.5 °F) |
| Flash Point | 2 °C (35.6 °F (closed cup)) |
| Vapor Pressure | 60.4 mmHg (25 °C) |
| Water Solubility | 31 g/L (20 °C) |
| pH / pKa | Neutral ester |
| Viscosity | 0.52 mPa·s (25 °C) |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
GHS Classification & Precautions
- H225: Highly flammable liquid and vapor
- H319: Causes serious eye irritation
- H336: May cause drowsiness or dizziness
- P210: Keep away from heat, sparks, and open flames
- P240: Ground and bond container and receiving equipment
Handling & storage: Store in grounded flammable cabinets away from strong bases/oxidizers. Attacks amorphous polymers (ABS, PC, PVC-U, PMMA); use PTFE, FEP, PFA, PEEK, or PPS.
Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25
Plastics in Contact with Isopropyl Acetate
Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.
| Plastic Family | Rating & Conditions | Engineering Notes |
|---|---|---|
| Polypropylene (PP)
ISO 1043: PP | Good resistance to Isopropyl Acetate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C) | |
| High-Density Polyethylene (HDPE)
ISO 1043: PE-HD | Good resistance to Isopropyl Acetate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: High-density polyethylene (PE100 / blow-molding HDPE) | |
| Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS | Not recommended: Isopropyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in ABS even under short-term contact. Grade basis: General-purpose unreinforced ABS molding grade | |
| Polycarbonate (PC)
ISO 1043: PC | Not recommended: Isopropyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact. Grade basis: Unfilled bisphenol-A polycarbonate (PC) | |
| Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66 | Excellent resistance to Isopropyl Acetate at 20 °C with negligible swelling, weight change, or mechanical degradation in PA66 (Nylon 66). Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66) | |
| Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD | Good resistance to Isopropyl Acetate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade) | |
| Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U | Not recommended: Isopropyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact. Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade) | |
| Polystyrene (GPPS) (PS)
ISO 1043: PS | Not recommended: Isopropyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact. Grade basis: General-purpose crystal polystyrene (GPPS) | |
| Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6 | Excellent resistance to Isopropyl Acetate at 20 °C with negligible swelling, weight change, or mechanical degradation in PA6 (Nylon 6). Grade basis: Unreinforced polyamide 6 (extruded/molded PA6) | |
| Polyoxymethylene (Acetal) (POM)
ISO 1043: POM | Good resistance to Isopropyl Acetate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H) | |
| Polybutylene Terephthalate (PBT)
ISO 1043: PBT | Good resistance to Isopropyl Acetate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Unreinforced polybutylene terephthalate (PBT) | |
| Polyethylene Terephthalate (PET)
ISO 1043: PET | Good resistance to Isopropyl Acetate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Semi-crystalline / oriented PET resin | |
| Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA | Not recommended: Isopropyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact. Grade basis: Cast & extruded polymethyl methacrylate (PMMA) | |
| Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW | Good resistance to Isopropyl Acetate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Virgin compression-molded UHMWPE (>3M g/mol) | |
| Styrene-Acrylonitrile (SAN)
ISO 1043: SAN | Not recommended: Isopropyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in SAN even under short-term contact. Grade basis: Transparent styrene-acrylonitrile copolymer (SAN) | |
| Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE | Virtually inert to Isopropyl Acetate at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade) | |
| Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF | Limited resistance to Isopropyl Acetate at 20 °C; moderate swelling, softening, or stress-cracking risk makes PVDF unsuitable for continuous containment. Grade basis: Homopolymer PVDF (pipe, valve & sheet grade) | |
| Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP | Virtually inert to Isopropyl Acetate at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: Melt-extruded FEP tubing & lining grade | |
| Polyether Ether Ketone (PEEK)
ISO 1043: PEEK | Excellent resistance to Isopropyl Acetate at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK. Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class) | |
| Polyphenylene Sulfide (PPS)
ISO 1043: PPS | Excellent resistance to Isopropyl Acetate at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS. Grade basis: Linear / 40% glass-filled PPS (PPS-GF40) | |
| Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA | Virtually inert to Isopropyl Acetate at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: High-purity melt-processable PFA tubing & lining grade | |
| Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM | Good resistance to Isopropyl Acetate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A) | |
| Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM | Not recommended: Isopropyl Acetate causes rapid swelling, softening, and seal failure in FKM (Viton) fluoroelastomer; consider EPDM or PTFE/FEP-encapsulated seals instead. Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine) | |
| Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR | Not recommended: Isopropyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact. Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N) | |
| Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ | Not recommended: Isopropyl Acetate causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact. Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ) |
Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25
Upstream, Downstream & Applications
- Esterification of isopropanol with acetic acid
- Direct addition of acetic acid to propylene
- Flexographic and gravure printing inks
- Pharmaceutical extraction and nitrocellulose coatings
- Solvent for flexographic/gravure packaging inks
- Coating solvent for plastics, cellulose, and synthetic resins
- Process extraction solvent in pharmaceuticals
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
Source Isopropyl Acetate & Compatible Equipment
High-purity industrial grade · Bulk supply
View Suppliers on Made-in-China.comHDPE / PTFE / FKM / EPDM solvent transfer equipment