Phenol
High-volume aromatic alcohol co-produced with acetone via the cumene process, serving as the essential feedstock for Bisphenol A (PC/epoxy), phenolic resins, and Nylon 6.
Also known as: Carbolic acid, Hydroxybenzene, Benzenol
Registry Numbers & Structural Strings
| Identifier | Value |
|---|---|
| CAS Registry Number | 108-95-2 |
| EC Number | 203-632-7 |
| Molecular Formula | C6H6O |
| Molecular Weight | 94.11 g/mol |
| IUPAC Name | phenol |
| Canonical SMILES | C1=CC=C(C=C1)O |
| InChI | InChI=1S/C6H6O/c7-6-4-2-1-3-5-6/h1-5,7H |
| InChIKey | ISWSIDIOOBJBQZ-UHFFFAOYSA-N |
| UN Transport Number | UN1671 |
| PubChem CID | 996 |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 996
Measured Constants (SI / Imperial)
Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Phenol (CAS 108-95-2) unless otherwise noted.
| Property | Value |
|---|---|
| Physical State | Solid (molten >41 °C) |
| Appearance | White crystalline mass (pink on air exposure) with sharp medicinal odor |
| Density | 1.071 g/cm³ (20 °C) (8.94 lb/gal) |
| Melting Point | 40.5 °C (104.9 °F) |
| Boiling Point | 181.7 °C (359.1 °F) |
| Flash Point | 79 °C (174.2 °F (closed cup)) |
| Vapor Pressure | 0.35 mmHg (25 °C) |
| Water Solubility | 83 g/L (20 °C) |
| pH / pKa | pKa 9.95 (weak acid) |
| Viscosity | 3.4 mPa·s (50 °C) |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
GHS Classification & Precautions
- H301+H311+H331: Toxic if swallowed, in contact with skin or inhaled
- H314: Causes severe skin burns and eye damage
- H341: Suspected of causing genetic defects
- P260: Do not breathe dust/vapors
- P280: Wear butyl/Viton gloves, apron, and full face shield
Handling & storage: Store tightly sealed away from light and oxidizers. Rapidly dissolves PA6/PA66, PC, ABS, PMMA, PS, PET, PBT, and attacks POM; restrict contact to PTFE, FEP, PFA, PVDF, PEEK, or FKM.
Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25
Plastics in Contact with Phenol
Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.
| Plastic Family | Rating & Conditions | Engineering Notes |
|---|---|---|
| Polypropylene (PP)
ISO 1043: PP | Good resistance to Phenol at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C) | |
| High-Density Polyethylene (HDPE)
ISO 1043: PE-HD | Good resistance to Phenol at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: High-density polyethylene (PE100 / blow-molding HDPE) | |
| Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in ABS even under short-term contact. Grade basis: General-purpose unreinforced ABS molding grade | |
| Polycarbonate (PC)
ISO 1043: PC | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact. Grade basis: Unfilled bisphenol-A polycarbonate (PC) | |
| Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66 | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in PA66 (Nylon 66) even under short-term contact. Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66) | |
| Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in LDPE even under short-term contact. Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade) | |
| Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact. Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade) | |
| Polystyrene (GPPS) (PS)
ISO 1043: PS | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact. Grade basis: General-purpose crystal polystyrene (GPPS) | |
| Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6 | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in PA6 (Nylon 6) even under short-term contact. Grade basis: Unreinforced polyamide 6 (extruded/molded PA6) | |
| Polyoxymethylene (Acetal) (POM)
ISO 1043: POM | Good resistance to Phenol at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H) | |
| Polybutylene Terephthalate (PBT)
ISO 1043: PBT | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in PBT even under short-term contact. Grade basis: Unreinforced polybutylene terephthalate (PBT) | |
| Polyethylene Terephthalate (PET)
ISO 1043: PET | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in PET even under short-term contact. Grade basis: Semi-crystalline / oriented PET resin | |
| Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact. Grade basis: Cast & extruded polymethyl methacrylate (PMMA) | |
| Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in UHMWPE even under short-term contact. Grade basis: Virgin compression-molded UHMWPE (>3M g/mol) | |
| Styrene-Acrylonitrile (SAN)
ISO 1043: SAN | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in SAN even under short-term contact. Grade basis: Transparent styrene-acrylonitrile copolymer (SAN) | |
| Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE | Virtually inert to Phenol at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade) | |
| Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF | Excellent resistance to Phenol at 20 °C with negligible swelling, weight change, or mechanical degradation in PVDF. Grade basis: Homopolymer PVDF (pipe, valve & sheet grade) | |
| Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP | Good resistance to Phenol at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Melt-extruded FEP tubing & lining grade | |
| Polyether Ether Ketone (PEEK)
ISO 1043: PEEK | Excellent resistance to Phenol at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK. Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class) | |
| Polyphenylene Sulfide (PPS)
ISO 1043: PPS | Excellent resistance to Phenol at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS. Grade basis: Linear / 40% glass-filled PPS (PPS-GF40) | |
| Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA | Virtually inert to Phenol at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: High-purity melt-processable PFA tubing & lining grade | |
| Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM | Limited resistance to Phenol at 20 °C; moderate swelling, softening, or stress-cracking risk makes EPDM rubber unsuitable for continuous containment. Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A) | |
| Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM | Excellent resistance to Phenol at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer. Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine) | |
| Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact. Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N) | |
| Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ | Not recommended: Phenol causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact. Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ) |
Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25
Upstream, Downstream & Applications
- Cumene hydroperoxide cleavage (co-product with acetone)
- Bisphenol A (BPA) -> Polycarbonate (PC) & Epoxy resins
- Phenolic (Bakelite) wood-panel and molding resins
- Caprolactam (PA6) and alkylphenols
- Key monomer for Bisphenol A (PC & epoxy resins) and phenolic resins
- Precursor for cyclohexanone/caprolactam (Nylon 6)
- Antiseptic, resin intermediate, and herbicide synthesis
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
Source Phenol & Compatible Equipment
High-purity industrial grade · Bulk supply
View Suppliers on Made-in-China.comVerified ISO-certified chemical manufacturers
View Suppliers on Made-in-China.com