CHEMICAL · CAS 109-99-9

Tetrahydrofuran (THF)

CAS 109-99-9 · EC 203-726-8 · C4H8O · UN2056

Water-miscible cyclic ether and one of the strongest industrial polymer solvents, essential for PVC pipe cements, PTMEG spandex production, and organometallic synthesis.

Also known as: Oxolane, Tetramethylene oxide, 1,4-Epoxybutane

Molecular Weight
72.11 g/mol
Boiling Point
66 °C
Melting Point
-108.4 °C
Flash Point
-14.5 °C
Density
0.8876 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Tetrahydrofuran (THF) chemical identifiers
Identifier Value
CAS Registry Number 109-99-9
EC Number 203-726-8
Molecular Formula C4H8O
Molecular Weight 72.11 g/mol
IUPAC Name oxolane
Canonical SMILES C1CCOC1
InChI InChI=1S/C4H8O/c1-2-4-5-3-1/h1-4H2
InChIKey WYURNTSHIVDZCO-UHFFFAOYSA-N
UN Transport Number UN2056
PubChem CID 8028

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 8028

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Tetrahydrofuran (THF) (CAS 109-99-9) unless otherwise noted.

Density (vs. Water = 1.0)0.8876 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-108.4 °C
-13020 °C260
Boiling Point66 °C
-50Water 100 °C350
Flash Point (Closed Cup)-14.5 °C
-50GHS Cat.2 (23 °C)220
Tetrahydrofuran (THF) physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless, mobile liquid with ethereal odor
Density 0.8876 g/cm³ (20 °C) (7.41 lb/gal)
Melting Point -108.4 °C (-163.1 °F)
Boiling Point 66 °C (150.8 °F)
Flash Point -14.5 °C (5.9 °F (closed cup))
Vapor Pressure 162 mmHg (25 °C)
Water Solubility Miscible in all proportions
pH / pKa Neutral (non-protic ether)
Viscosity 0.456 mPa·s (25 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS02 Flammable
GHS08 Health Hazard
GHS07 Irritant / Harmful
Flammable Liquids (Category 2) · Acute Toxicity — Oral (Category 4) · Serious Eye Irritation (Category 2A) · Carcinogenicity (Category 2)
Hazard statements
  • H225: Highly flammable liquid and vapor
  • H302: Harmful if swallowed
  • H319: Causes serious eye irritation
  • H351: Suspected of causing cancer
  • EUH019: May form explosive peroxides
Key precautionary statements
  • P210: Keep away from heat, sparks, open flames and hot surfaces
  • P233: Keep container tightly closed under nitrogen with BHT stabilizer
  • P280: Wear protective gloves and eye protection

Handling & storage: Store inhibited (BHT) under inert gas away from light to prevent explosive peroxide formation. Aggressively dissolves PVC, ABS, PC, PS, PMMA, and swells polyolefins; restrict wetted contact to PTFE, FEP, PEEK, or PPS.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Tetrahydrofuran (THF)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Tetrahydrofuran (THF)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to tetrahydrofuran (THF) at 20 °C; moderate swelling, softening, or stress-cracking risk makes polypropylene (PP) unsuitable for continuous pressurized containment.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to tetrahydrofuran (THF) at 20 °C; moderate swelling, softening, or stress-cracking risk makes HDPE unsuitable for continuous pressurized containment.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: tetrahydrofuran (THF) causes severe chemical attack, dissolution, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: tetrahydrofuran (THF) causes severe chemical attack, dissolution, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to tetrahydrofuran (THF) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PA66 (Nylon 66) unsuitable for continuous pressurized containment.
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to tetrahydrofuran (THF) at 20 °C; moderate swelling, softening, or stress-cracking risk makes LDPE unsuitable for continuous pressurized containment.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: tetrahydrofuran (THF) causes severe chemical attack, dissolution, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: tetrahydrofuran (THF) causes severe chemical attack, dissolution, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to tetrahydrofuran (THF) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA6 (Nylon 6).
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to tetrahydrofuran (THF) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to tetrahydrofuran (THF) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PBT unsuitable for continuous pressurized containment.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to tetrahydrofuran (THF) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PET unsuitable for continuous pressurized containment.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: tetrahydrofuran (THF) causes severe chemical attack, dissolution, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to tetrahydrofuran (THF) at 20 °C; moderate swelling, softening, or stress-cracking risk makes UHMWPE unsuitable for continuous pressurized containment.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: tetrahydrofuran (THF) causes severe chemical attack, dissolution, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to tetrahydrofuran (THF) at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to tetrahydrofuran (THF) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PVDF.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to tetrahydrofuran (THF) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to tetrahydrofuran (THF) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to tetrahydrofuran (THF) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Tetrahydrofuran (THF) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Tetrahydrofuran (THF) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Tetrahydrofuran (THF) causes rapid swelling, softening, and seal failure in FKM (Viton) fluoroelastomer; consider EPDM or PTFE/FEP-encapsulated seals instead.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Tetrahydrofuran (THF) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Tetrahydrofuran (THF) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Acid-catalyzed dehydration of 1,4-butanediol (BDO)
  • Hydrogenation of maleic anhydride or furan
Downstream Derivatives
  • Polytetramethylene ether glycol (PTMEG) for elastane/spandex and TPU
  • PVC/CPVC pipe solvent cements and coating resins
Typical Industrial Uses
  • Monomer for PTMEG polyurethane elastomers and spandex fibers
  • Primary solvent in rigid PVC and CPVC pipe welding cements
  • Reaction medium for Grignard, organolithium, and pharmaceutical synthesis

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Tetrahydrofuran (THF) & Compatible Equipment

Tetrahydrofuran Industrial / Reagent Grade (CAS 109-99-9)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Solvent-Resistant Chemical Drums, Pumps & Seals