CHEMICAL · CAS 110-54-3

n-Hexane

CAS 110-54-3 · EC 203-777-6 · C6H14 · UN1208

Non-polar, low-boiling six-carbon alkane used extensively for vegetable oil extraction, rubber/shoe adhesive formulation, polyolefin polymerization diluent, and laboratory chromatography.

Also known as: Hexane, Normal hexane, Skellysolve B

Molecular Weight
86.18 g/mol
Boiling Point
68.7 °C
Melting Point
-95.3 °C
Flash Point
-22 °C
Density
0.6594 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

n-Hexane chemical identifiers
Identifier Value
CAS Registry Number 110-54-3
EC Number 203-777-6
Molecular Formula C6H14
Molecular Weight 86.18 g/mol
IUPAC Name hexane
Canonical SMILES CCCCCC
InChI InChI=1S/C6H14/c1-3-5-6-4-2/h3-6H2,1-2H3
InChIKey VLKZOEOYAKHREP-UHFFFAOYSA-N
UN Transport Number UN1208
PubChem CID 8058

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 8058

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous n-Hexane (CAS 110-54-3) unless otherwise noted.

Density (vs. Water = 1.0)0.6594 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-95.3 °C
-13020 °C260
Boiling Point68.7 °C
-50Water 100 °C350
Flash Point (Closed Cup)-22 °C
-50GHS Cat.2 (23 °C)220
n-Hexane physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless volatile liquid with mild petroleum odor
Density 0.6594 g/cm³ (20 °C) (5.50 lb/gal)
Melting Point -95.3 °C (-139.5 °F)
Boiling Point 68.7 °C (155.7 °F)
Flash Point -22 °C (-7.6 °F (closed cup))
Vapor Pressure 151 mmHg (25 °C)
Water Solubility 0.0095 g/L (25 °C, virtually insoluble)
pH / pKa Non-polar aliphatic alkane
Viscosity 0.297 mPa·s (25 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS02 Flammable
GHS06 Acute Toxicity
GHS08 Health Hazard
Flammable Liquids (Category 2) · Aspiration Hazard (Category 1) · Reproductive Toxicity (Category 2) · STOT — Repeated Exposure (Category 2, peripheral neuropathy)
Hazard statements
  • H225: Highly flammable liquid and vapor
  • H304: May be fatal if swallowed and enters airways
  • H361f: Suspected of damaging fertility
  • H373: May cause damage to peripheral nervous system through prolonged inhalation
Key precautionary statements
  • P210: Keep away from heat, sparks, open flames and hot surfaces
  • P240: Ground and bond container and receiving equipment
  • P260: Do not breathe vapors

Handling & storage: Store in grounded, explosion-proof flammable storage; vapors are heavier than air. Compatible with PTFE, PVDF, FEP, PA66, POM, PEEK, and PVC-U; causes gradual swelling/permeation in LDPE, HDPE, PP, and PS.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with n-Hexane

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with n-Hexane
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-hexane at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-hexane at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-hexane at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to n-hexane at 20 °C; moderate swelling, softening, or stress-cracking risk makes polycarbonate (PC) unsuitable for continuous pressurized containment.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-hexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA66 (Nylon 66).
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to n-hexane at 20 °C; moderate swelling, softening, or stress-cracking risk makes LDPE unsuitable for continuous pressurized containment.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-hexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed rigid PVC (PVC-U).
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-hexane causes severe chemical attack, dissolution, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-hexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA6 (Nylon 6).
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-hexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed acetal (POM).
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-hexane at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-hexane at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to n-hexane at 20 °C; moderate swelling, softening, or stress-cracking risk makes acrylic (PMMA) unsuitable for continuous pressurized containment.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-hexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed UHMWPE.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to n-hexane at 20 °C; moderate swelling, softening, or stress-cracking risk makes SAN unsuitable for continuous pressurized containment.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to n-hexane at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-hexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PVDF.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to n-hexane at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-hexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-hexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to n-Hexane at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Hexane severely swells and degrades EPDM rubber; specify FKM (Viton) or PTFE/PFA seals for hydrocarbon or strong-acid service.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-Hexane at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-Hexane at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Hexane causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Fractional distillation of crude oil naphtha and natural gas condensates
Downstream Derivatives
  • Edible oilseed extraction (soybean, canola)
  • Rubber contact cements and polyolefin slurry polymerization
Typical Industrial Uses
  • Solvent extraction of vegetable oils from seeds
  • Diluent in HDPE and PP Ziegler-Natta polymerization reactors
  • Fast-drying solvent in rubber adhesives, coatings, and HPLC

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source n-Hexane & Compatible Equipment

n-Hexane Industrial / Reagent Grade (CAS 110-54-3)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Solvent-Resistant Chemical Drums, Pumps & Seals