Cyclohexane
Non-polar six-membered cycloalkane serving primarily as the industrial feedstock for nylon-6 (caprolactam) and nylon-66 (adipic acid) intermediates, as well as a low-toxicity substitute for n-hexane.
Also known as: Hexamethylene, Hexahydrobenzene, Naphthene
Registry Numbers & Structural Strings
| Identifier | Value |
|---|---|
| CAS Registry Number | 110-82-7 |
| EC Number | 203-806-2 |
| Molecular Formula | C6H12 |
| Molecular Weight | 84.16 g/mol |
| IUPAC Name | cyclohexane |
| Canonical SMILES | C1CCCCC1 |
| InChI | InChI=1S/C6H12/c1-2-4-6-5-3-1/h1-6H2 |
| InChIKey | XDTMQSROBMDMFD-UHFFFAOYSA-N |
| UN Transport Number | UN1145 |
| PubChem CID | 8078 |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 8078
Measured Constants (SI / Imperial)
Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Cyclohexane (CAS 110-82-7) unless otherwise noted.
| Property | Value |
|---|---|
| Physical State | Liquid |
| Appearance | Colorless mobile liquid with mild sweet-petroleum odor |
| Density | 0.7785 g/cm³ (20 °C) (6.50 lb/gal) |
| Melting Point | 6.5 °C (43.7 °F) |
| Boiling Point | 80.7 °C (177.3 °F) |
| Flash Point | -20 °C (-4 °F (closed cup)) |
| Vapor Pressure | 97.6 mmHg (25 °C) |
| Water Solubility | 0.055 g/L (25 °C) |
| pH / pKa | Non-polar cycloalkane |
| Viscosity | 0.894 mPa·s (25 °C) |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
GHS Classification & Precautions
- H225: Highly flammable liquid and vapor
- H304: May be fatal if swallowed and enters airways
- H336: May cause drowsiness or dizziness
- H410: Very toxic to aquatic life with long lasting effects
- P210: Keep away from heat, sparks, open flames and hot surfaces
- P273: Avoid release to the environment
- P301+P310: IF SWALLOWED: Immediately call a poison center
Handling & storage: Keep grounded above 10 °C if freezing in transfer lines is a concern. Compatible with PTFE, PVDF, FEP, PA66, POM, PBT, and PEEK; swells polyolefins (PP/PE) and attacks PS.
Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25
Plastics in Contact with Cyclohexane
Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.
| Plastic Family | Rating & Conditions | Engineering Notes |
|---|---|---|
| Polypropylene (PP)
ISO 1043: PP | Limited resistance to cyclohexane at 20 °C; moderate swelling, softening, or stress-cracking risk makes polypropylene (PP) unsuitable for continuous pressurized containment. Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C) | |
| High-Density Polyethylene (HDPE)
ISO 1043: PE-HD | Limited resistance to cyclohexane at 20 °C; moderate swelling, softening, or stress-cracking risk makes HDPE unsuitable for continuous pressurized containment. Grade basis: High-density polyethylene (PE100 / blow-molding HDPE) | |
| Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS | Good resistance to cyclohexane at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: General-purpose unreinforced ABS molding grade | |
| Polycarbonate (PC)
ISO 1043: PC | Limited resistance to cyclohexane at 20 °C; moderate swelling, softening, or stress-cracking risk makes polycarbonate (PC) unsuitable for continuous pressurized containment. Grade basis: Unfilled bisphenol-A polycarbonate (PC) | |
| Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66 | Excellent resistance to cyclohexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA66 (Nylon 66). Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66) | |
| Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD | Limited resistance to cyclohexane at 20 °C; moderate swelling, softening, or stress-cracking risk makes LDPE unsuitable for continuous pressurized containment. Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade) | |
| Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U | Excellent resistance to cyclohexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed rigid PVC (PVC-U). Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade) | |
| Polystyrene (GPPS) (PS)
ISO 1043: PS | Not recommended: cyclohexane causes severe chemical attack, dissolution, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact. Grade basis: General-purpose crystal polystyrene (GPPS) | |
| Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6 | Excellent resistance to cyclohexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA6 (Nylon 6). Grade basis: Unreinforced polyamide 6 (extruded/molded PA6) | |
| Polyoxymethylene (Acetal) (POM)
ISO 1043: POM | Excellent resistance to cyclohexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed acetal (POM). Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H) | |
| Polybutylene Terephthalate (PBT)
ISO 1043: PBT | Good resistance to cyclohexane at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Unreinforced polybutylene terephthalate (PBT) | |
| Polyethylene Terephthalate (PET)
ISO 1043: PET | Good resistance to cyclohexane at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Semi-crystalline / oriented PET resin | |
| Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA | Limited resistance to cyclohexane at 20 °C; moderate swelling, softening, or stress-cracking risk makes acrylic (PMMA) unsuitable for continuous pressurized containment. Grade basis: Cast & extruded polymethyl methacrylate (PMMA) | |
| Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW | Excellent resistance to cyclohexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed UHMWPE. Grade basis: Virgin compression-molded UHMWPE (>3M g/mol) | |
| Styrene-Acrylonitrile (SAN)
ISO 1043: SAN | Limited resistance to cyclohexane at 20 °C; moderate swelling, softening, or stress-cracking risk makes SAN unsuitable for continuous pressurized containment. Grade basis: Transparent styrene-acrylonitrile copolymer (SAN) | |
| Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE | Virtually inert to cyclohexane at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media. Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade) | |
| Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF | Excellent resistance to cyclohexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PVDF. Grade basis: Homopolymer PVDF (pipe, valve & sheet grade) | |
| Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP | Virtually inert to cyclohexane at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media. Grade basis: Melt-extruded FEP tubing & lining grade | |
| Polyether Ether Ketone (PEEK)
ISO 1043: PEEK | Excellent resistance to cyclohexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PEEK. Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class) | |
| Polyphenylene Sulfide (PPS)
ISO 1043: PPS | Excellent resistance to cyclohexane at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PPS. Grade basis: Linear / 40% glass-filled PPS (PPS-GF40) | |
| Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA | Virtually inert to Cyclohexane at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: High-purity melt-processable PFA tubing & lining grade | |
| Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM | Not recommended: Cyclohexane severely swells and degrades EPDM rubber; specify FKM (Viton) or PTFE/PFA seals for hydrocarbon or strong-acid service. Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A) | |
| Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM | Excellent resistance to Cyclohexane at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer. Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine) | |
| Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR | Excellent resistance to Cyclohexane at 20 °C with negligible swelling, weight change, or mechanical degradation in NBR (Buna-N) nitrile rubber. Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N) | |
| Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ | Not recommended: Cyclohexane causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact. Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ) |
Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25
Upstream, Downstream & Applications
- Catalytic hydrogenation of benzene
- Fractional distillation of straight-run naphtha
- KA oil (cyclohexanol/cyclohexanone) for caprolactam (PA6) and adipic acid (PA66)
- Rubber and adhesive solvent formulations
- Primary petrochemical precursor for Nylon 6 (PA6) and Nylon 66 (PA66)
- Solvent for SBS/SEBS thermoplastic elastomers, lacquers, and resins
- Recrystallization and extraction solvent
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
Source Cyclohexane & Compatible Equipment
High-purity industrial grade · Bulk supply
View Suppliers on Made-in-China.comHDPE / PTFE / FKM / EPDM solvent transfer equipment
View Suppliers on Made-in-China.com