CHEMICAL · CAS 121-44-8

Triethylamine (Et3N)

CAS 121-44-8 · EC 204-469-4 · C6H15N · UN1296

Volatile tertiary aliphatic amine widely used as an acid scavenger in pharmaceutical and polymer synthesis and as a curing catalyst in metal-casting foundries.

Also known as: N,N-Diethylethanamine, TEA (Tertiary Amine)

Molecular Weight
101.19 g/mol
Boiling Point
89.3 °C
Melting Point
-114.7 °C
Flash Point
-11 °C
Density
0.7255 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Triethylamine (Et3N) chemical identifiers
Identifier Value
CAS Registry Number 121-44-8
EC Number 204-469-4
Molecular Formula C6H15N
Molecular Weight 101.19 g/mol
IUPAC Name N,N-diethylethanamine
Canonical SMILES CCN(CC)CC
InChI InChI=1S/C6H15N/c1-4-7(5-2)6-3/h4-6H2,1-3H3
InChIKey ZMANZCXQSJIPKH-UHFFFAOYSA-N
UN Transport Number UN1296
PubChem CID 8471

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 8471

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Triethylamine (Et3N) (CAS 121-44-8) unless otherwise noted.

Density (vs. Water = 1.0)0.7255 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-114.7 °C
-13020 °C260
Boiling Point89.3 °C
-50Water 100 °C350
Flash Point (Closed Cup)-11 °C
-50GHS Cat.2 (23 °C)220
Triethylamine (Et3N) physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless volatile liquid with strong fishy ammoniacal odor
Density 0.7255 g/cm³ (20 °C) (6.05 lb/gal)
Melting Point -114.7 °C (-174.5 °F)
Boiling Point 89.3 °C (192.7 °F)
Flash Point -11 °C (12.2 °F (closed cup))
Vapor Pressure 57.1 mmHg (25 °C)
Water Solubility 112 g/L (20 °C)
pH / pKa pKa (conj. acid) 10.75
Viscosity 0.347 mPa·s (25 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS02 Flammable
GHS05 Corrosive
GHS06 Acute Toxicity
GHS07 Irritant / Harmful
Flammable Liquids (Cat. 2) · Acute Toxicity — Oral/Dermal/Inhalation (Cat. 3–4) · Skin Corrosion (Cat. 1A)
Hazard statements
  • H225: Highly flammable liquid and vapor
  • H302: Harmful if swallowed
  • H311+H331: Toxic in contact with skin or if inhaled
  • H314: Causes severe skin burns
Key precautionary statements
  • P210: Keep away from heat, sparks, and open flames
  • P280: Wear butyl gloves, eye/face protection, and fume hood

Handling & storage: Store in grounded flammable cabinets away from acids and oxidizers. Attacks PC, PVC-U, ABS, PMMA, and FKM; compatible with PTFE, FEP, PFA, PEEK, PPS, and ambient HDPE/PP.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Triethylamine (Et3N)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Triethylamine (Et3N)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethylamine (Et3N) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethylamine (Et3N) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethylamine (Et3N) causes severe attack, swelling, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethylamine (Et3N) causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethylamine (Et3N) at 20 °C with negligible swelling, weight change, or mechanical degradation in PA66 (Nylon 66).
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethylamine (Et3N) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethylamine (Et3N) causes severe attack, swelling, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethylamine (Et3N) causes severe attack, swelling, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethylamine (Et3N) at 20 °C with negligible swelling, weight change, or mechanical degradation in PA6 (Nylon 6).
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethylamine (Et3N) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Triethylamine (Et3N) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PBT unsuitable for continuous containment.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Triethylamine (Et3N) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PET unsuitable for continuous containment.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethylamine (Et3N) causes severe attack, swelling, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethylamine (Et3N) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethylamine (Et3N) causes severe attack, swelling, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Triethylamine (Et3N) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethylamine (Et3N) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Triethylamine (Et3N) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethylamine (Et3N) at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Triethylamine (Et3N) at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Triethylamine (Et3N) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Triethylamine (Et3N) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethylamine (Et3N) causes rapid swelling, softening, and seal failure in FKM (Viton) fluoroelastomer; consider EPDM or PTFE/FEP-encapsulated seals instead.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Triethylamine (Et3N) at 20 °C; moderate swelling, softening, or stress-cracking risk makes NBR (Buna-N) nitrile rubber unsuitable for continuous containment.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Triethylamine (Et3N) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Catalytic amination of ethanol with ammonia
Downstream Derivatives
  • Foundry cold-box polyurethane core curing catalyst
  • Acid scavenger in polycarbonate, pharmaceutical, and agrochemical synthesis
Typical Industrial Uses
  • Gaseous curing catalyst in automotive foundry sand-core production
  • Base catalyst and HCl scavenger in pharmaceutical and polycarbonate synthesis
  • Precursor for quaternary ammonium surfactants and waterborne PU neutralizers

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Triethylamine (Et3N) & Compatible Equipment

Triethylamine Industrial / Reagent Grade (CAS 121-44-8)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Triethylamine Bulk Chemical Suppliers & Packaging

Verified ISO-certified chemical manufacturers

View Suppliers on Made-in-China.com