Adipic Acid
Six-carbon dicarboxylic acid serving as the primary monomer for Nylon 66 (PA66), polyurethane polyester polyols, and PBAT biodegradable polymers.
Also known as: Hexanedioic acid, 1,4-Butanedicarboxylic acid, ADA
Registry Numbers & Structural Strings
| Identifier | Value |
|---|---|
| CAS Registry Number | 124-04-9 |
| EC Number | 204-673-3 |
| Molecular Formula | C6H10O4 |
| Molecular Weight | 146.14 g/mol |
| IUPAC Name | hexanedioic acid |
| Canonical SMILES | C(CCC(=O)O)CC(=O)O |
| InChI | InChI=1S/C6H10O4/c7-5(8)3-1-2-4-6(9)10/h1-4H2,(H,7,8)(H,9,10) |
| InChIKey | WNLRTRBMVRJNCN-UHFFFAOYSA-N |
| UN Transport Number | — |
| PubChem CID | 196 |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 196
Measured Constants (SI / Imperial)
Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Adipic Acid (CAS 124-04-9) unless otherwise noted.
| Property | Value |
|---|---|
| Physical State | Solid |
| Appearance | White crystalline odorless powder |
| Density | 1.36 g/cm³ (25 °C) (11.35 lb/gal) |
| Melting Point | 152.1 °C (305.8 °F) |
| Boiling Point | 337.5 °C (639.5 °F) |
| Flash Point | 196 °C (384.8 °F (closed cup)) |
| Vapor Pressure | <0.001 mmHg (25 °C) |
| Water Solubility | 14.4 g/L (15 °C) |
| pH / pKa | pKa1 4.41, pKa2 5.41 |
| Viscosity | — |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
GHS Classification & Precautions
- H319: Causes serious eye irritation
- P264: Wash hands thoroughly after handling
- P280: Wear eye protection and dust mask
Handling & storage: Store in dry, dust-controlled bags/silos away from strong alkalis. Compatible with PP, HDPE, LDPE, PVC-U, PTFE, PVDF, and PEEK.
Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25
Plastics in Contact with Adipic Acid
Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.
| Plastic Family | Rating & Conditions | Engineering Notes |
|---|---|---|
| Polypropylene (PP)
ISO 1043: PP | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in polypropylene (PP). Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C) | |
| High-Density Polyethylene (HDPE)
ISO 1043: PE-HD | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in HDPE. Grade basis: High-density polyethylene (PE100 / blow-molding HDPE) | |
| Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in ABS. Grade basis: General-purpose unreinforced ABS molding grade | |
| Polycarbonate (PC)
ISO 1043: PC | Good resistance to Adipic Acid at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Unfilled bisphenol-A polycarbonate (PC) | |
| Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66 | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in PA66 (Nylon 66). Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66) | |
| Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in LDPE. Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade) | |
| Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in rigid PVC (PVC-U). Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade) | |
| Polystyrene (GPPS) (PS)
ISO 1043: PS | Good resistance to Adipic Acid at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: General-purpose crystal polystyrene (GPPS) | |
| Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6 | Good resistance to Adipic Acid at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Unreinforced polyamide 6 (extruded/molded PA6) | |
| Polyoxymethylene (Acetal) (POM)
ISO 1043: POM | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in acetal (POM). Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H) | |
| Polybutylene Terephthalate (PBT)
ISO 1043: PBT | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in PBT. Grade basis: Unreinforced polybutylene terephthalate (PBT) | |
| Polyethylene Terephthalate (PET)
ISO 1043: PET | Good resistance to Adipic Acid at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Semi-crystalline / oriented PET resin | |
| Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in acrylic (PMMA). Grade basis: Cast & extruded polymethyl methacrylate (PMMA) | |
| Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in UHMWPE. Grade basis: Virgin compression-molded UHMWPE (>3M g/mol) | |
| Styrene-Acrylonitrile (SAN)
ISO 1043: SAN | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in SAN. Grade basis: Transparent styrene-acrylonitrile copolymer (SAN) | |
| Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE | Good resistance to Adipic Acid at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade) | |
| Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in PVDF. Grade basis: Homopolymer PVDF (pipe, valve & sheet grade) | |
| Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP | Virtually inert to Adipic Acid at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: Melt-extruded FEP tubing & lining grade | |
| Polyether Ether Ketone (PEEK)
ISO 1043: PEEK | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK. Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class) | |
| Polyphenylene Sulfide (PPS)
ISO 1043: PPS | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS. Grade basis: Linear / 40% glass-filled PPS (PPS-GF40) | |
| Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA | Virtually inert to Adipic Acid at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: High-purity melt-processable PFA tubing & lining grade | |
| Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in EPDM rubber. Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A) | |
| Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer. Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine) | |
| Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR | Good resistance to Adipic Acid at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N) | |
| Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ | Excellent resistance to Adipic Acid at 20 °C with negligible swelling, weight change, or mechanical degradation in VMQ silicone rubber. Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ) |
Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25
Upstream, Downstream & Applications
- Nitric acid oxidation of cyclohexanol/cyclohexanone (KA oil)
- Polyamide 66 (PA66 / Nylon 66) engineering plastics and airbag/tire yarns
- Polyester polyols for TPU/shoe-sole polyurethanes and adipate plasticizers (DOA)
- Co-monomer with hexamethylenediamine for Nylon 66 (PA66)
- Feedstock for polyurethane polyester polyols (TPU/footwear)
- Precursor for low-temperature PVC plasticizers (DOA) and PBAT biodegradable plastics
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
Source Adipic Acid & Compatible Equipment
High-purity industrial grade · Bulk supply
View Suppliers on Made-in-China.comVerified ISO-certified chemical manufacturers
View Suppliers on Made-in-China.com