Potassium Hydroxide (KOH)
Strong, highly soluble inorganic base used in alkaline battery electrolytes, potassium carbonate/phosphate synthesis, liquid soap saponification, and anisotropic silicon wafer etching.
Also known as: Caustic potash, Potash lye, Potassium hydrate
Registry Numbers & Structural Strings
| Identifier | Value |
|---|---|
| CAS Registry Number | 1310-58-3 |
| EC Number | 215-181-3 |
| Molecular Formula | HKO |
| Molecular Weight | 56.11 g/mol |
| IUPAC Name | potassium hydroxide |
| Canonical SMILES | [OH-].[K+] |
| InChI | InChI=1S/K.H2O/h;1H2/q+1;/p-1 |
| InChIKey | KWYUFKZDYYNOTN-UHFFFAOYSA-M |
| UN Transport Number | UN1813 |
| PubChem CID | 14797 |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 14797
Measured Constants (SI / Imperial)
CAS identifiers and melting/boiling points refer to pure KOH flakes; viscosity and compatibility ratings reflect 45–50% w/w aqueous caustic potash.
| Property | Value |
|---|---|
| Physical State | Solid (or 45–50% aqueous solution) |
| Appearance | White deliquescent flakes/pellets or clear viscous aqueous solution |
| Density | 2.044 g/cm³ (solid); 1.45 g/cm³ (45% aq.) (12.10 lb/gal (45% aq.)) |
| Melting Point | 360 °C (680 °F) |
| Boiling Point | 1327 °C (2420.6 °F) |
| Flash Point | — |
| Vapor Pressure | Negligible (solid) |
| Water Solubility | 1,210 g/L (25 °C, strongly exothermic) |
| pH / pKa | pH ~14 (1 M aqueous) |
| Viscosity | 5.6 mPa·s (45% aq., 20 °C) |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
GHS Classification & Precautions
- H290: May be corrosive to metals (Al, Zn, Sn)
- H302: Harmful if swallowed
- H314: Causes severe skin burns and eye damage
- P260: Do not breathe dust or mist
- P280: Wear alkali-resistant gloves and face shield
- P305+P351+P338: IF IN EYES: Rinse cautiously with water
Handling & storage: Store in airtight, moisture-proof PP, HDPE, or PTFE vessels (absorbs atmospheric CO2 and water). Attacks PC, PET, PBT, and hot PVDF; compatible with PP, HDPE, LDPE, UHMWPE, PTFE, FEP, and PEEK.
Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25
Plastics in Contact with Potassium Hydroxide (KOH)
Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.
| Plastic Family | Rating & Conditions | Engineering Notes |
|---|---|---|
| Polypropylene (PP)
ISO 1043: PP | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed polypropylene (PP). Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C) | |
| High-Density Polyethylene (HDPE)
ISO 1043: PE-HD | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed HDPE. Grade basis: High-density polyethylene (PE100 / blow-molding HDPE) | |
| Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed ABS. Grade basis: General-purpose unreinforced ABS molding grade | |
| Polycarbonate (PC)
ISO 1043: PC | Not recommended: concentrated potassium hydroxide (KOH) causes severe chemical attack, dissolution, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact. Grade basis: Unfilled bisphenol-A polycarbonate (PC) | |
| Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66 | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA66 (Nylon 66). Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66) | |
| Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed LDPE. Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade) | |
| Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed rigid PVC (PVC-U). Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade) | |
| Polystyrene (GPPS) (PS)
ISO 1043: PS | Good resistance to concentrated potassium hydroxide (KOH) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: General-purpose crystal polystyrene (GPPS) | |
| Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6 | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA6 (Nylon 6). Grade basis: Unreinforced polyamide 6 (extruded/molded PA6) | |
| Polyoxymethylene (Acetal) (POM)
ISO 1043: POM | Good resistance to concentrated potassium hydroxide (KOH) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H) | |
| Polybutylene Terephthalate (PBT)
ISO 1043: PBT | Not recommended: concentrated potassium hydroxide (KOH) causes severe chemical attack, dissolution, crazing, or rapid structural failure in PBT even under short-term contact. Grade basis: Unreinforced polybutylene terephthalate (PBT) | |
| Polyethylene Terephthalate (PET)
ISO 1043: PET | Not recommended: concentrated potassium hydroxide (KOH) causes severe chemical attack, dissolution, crazing, or rapid structural failure in PET even under short-term contact. Grade basis: Semi-crystalline / oriented PET resin | |
| Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed acrylic (PMMA). Grade basis: Cast & extruded polymethyl methacrylate (PMMA) | |
| Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed UHMWPE. Grade basis: Virgin compression-molded UHMWPE (>3M g/mol) | |
| Styrene-Acrylonitrile (SAN)
ISO 1043: SAN | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed SAN. Grade basis: Transparent styrene-acrylonitrile copolymer (SAN) | |
| Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE | Good resistance to concentrated potassium hydroxide (KOH) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade) | |
| Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PVDF. Grade basis: Homopolymer PVDF (pipe, valve & sheet grade) | |
| Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP | Good resistance to concentrated potassium hydroxide (KOH) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Melt-extruded FEP tubing & lining grade | |
| Polyether Ether Ketone (PEEK)
ISO 1043: PEEK | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PEEK. Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class) | |
| Polyphenylene Sulfide (PPS)
ISO 1043: PPS | Excellent resistance to concentrated potassium hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PPS. Grade basis: Linear / 40% glass-filled PPS (PPS-GF40) | |
| Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA | Virtually inert to Potassium Hydroxide (KOH) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: High-purity melt-processable PFA tubing & lining grade | |
| Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM | Excellent resistance to Potassium Hydroxide (KOH) at 20 °C with negligible swelling, weight change, or mechanical degradation in EPDM rubber. Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A) | |
| Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM | Good resistance to Potassium Hydroxide (KOH) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine) | |
| Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR | Good resistance to Potassium Hydroxide (KOH) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N) | |
| Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ | Limited resistance to Potassium Hydroxide (KOH) at 20 °C; moderate swelling, softening, or stress-cracking risk makes VMQ silicone rubber unsuitable for continuous containment. Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ) |
Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25
Upstream, Downstream & Applications
- Membrane-cell chlor-alkali electrolysis of potassium chloride (KCl) brine
- Alkaline manganese and nickel-cadmium battery electrolytes
- Potassium fertilizers, liquid soaps, and biodiesel catalysts
- Semiconductor/MEMS anisotropic silicon wet etching
- Electrolyte in alkaline batteries and alkaline water electrolyzers (green H2)
- Anisotropic etching of silicon wafers in MEMS and solar cell fabrication
- Liquid potassium soaps, CO2 scrubbing, and chemical synthesis
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
Source Potassium Hydroxide (KOH) & Compatible Equipment
Anhydrous Solid / 45–50% Aqueous Basis · Bulk drums / IBCs
View Suppliers on Made-in-China.comPP-H / HDPE / PVDF / PTFE-lined chemical tanks & valves
View Suppliers on Made-in-China.com