Molecular Weight
128.17 g/mol
Boiling Point
145 °C
Melting Point
-64.6 °C
Flash Point
39 °C
Density
0.894 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

n-Butyl Acrylate chemical identifiers
Identifier Value
CAS Registry Number 141-32-2
EC Number 205-480-7
Molecular Formula C7H12O2
Molecular Weight 128.17 g/mol
IUPAC Name butyl prop-2-enoate
Canonical SMILES CCCCOC(=O)C=C
InChI InChI=1S/C7H12O2/c1-3-5-6-9-7(8)4-2/h4H,2-3,5-6H2,1H3
InChIKey CQEYYJKEWSMYFG-UHFFFAOYSA-N
UN Transport Number UN2348
PubChem CID 8846

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 8846

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous n-Butyl Acrylate (CAS 141-32-2) unless otherwise noted.

Density (vs. Water = 1.0)0.894 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-64.6 °C
-13020 °C260
Boiling Point145 °C
-50Water 100 °C350
Flash Point (Closed Cup)39 °C
-50GHS Cat.2 (23 °C)220
n-Butyl Acrylate physical and chemical properties
Property Value
Physical State Liquid
Appearance Clear, colorless liquid with sharp fruity-acrylic odor
Density 0.894 g/cm³ (20 °C) (7.46 lb/gal)
Melting Point -64.6 °C (-84.3 °F)
Boiling Point 145 °C (293 °F)
Flash Point 39 °C (102.2 °F (closed cup))
Vapor Pressure 5.45 mmHg (25 °C)
Water Solubility 1.4 g/L (20 °C)
pH / pKa Neutral unsaturated ester
Viscosity 0.88 mPa·s (20 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Warning
GHS02 Flammable
GHS07 Irritant / Harmful
Flammable Liquids (Cat. 3) · Skin/Eye Irritation (Cat. 2) · Skin Sensitization (Cat. 1) · STOT — Single Exposure (Cat. 3)
Hazard statements
  • H226: Flammable liquid and vapor
  • H315+H319: Causes skin and serious eye irritation
  • H317: May cause an allergic skin reaction
  • H335: May cause respiratory irritation
Key precautionary statements
  • P210: Keep away from heat and ignition sources
  • P280: Wear protective gloves and eye protection

Handling & storage: Store inhibited with MEHQ under air headspace below 30 °C. Attacks ABS, PC, PS, PMMA, PVC-U, EPDM, and NBR; specify PTFE, FEP, PFA, PEEK, or PPS.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with n-Butyl Acrylate

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with n-Butyl Acrylate
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-Butyl Acrylate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-Butyl Acrylate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acrylate causes severe attack, swelling, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acrylate causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-Butyl Acrylate at 20 °C with negligible swelling, weight change, or mechanical degradation in PA66 (Nylon 66).
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-Butyl Acrylate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acrylate causes severe attack, swelling, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acrylate causes severe attack, swelling, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-Butyl Acrylate at 20 °C with negligible swelling, weight change, or mechanical degradation in PA6 (Nylon 6).
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-Butyl Acrylate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-Butyl Acrylate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-Butyl Acrylate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acrylate causes severe attack, swelling, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-Butyl Acrylate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acrylate causes severe attack, swelling, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to n-Butyl Acrylate at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to n-Butyl Acrylate at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to n-Butyl Acrylate at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-Butyl Acrylate at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to n-Butyl Acrylate at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to n-Butyl Acrylate at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acrylate severely swells and degrades EPDM rubber; specify FKM (Viton) or PTFE/PFA seals for hydrocarbon or strong-acid service.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acrylate causes rapid swelling, softening, and seal failure in FKM (Viton) fluoroelastomer; consider EPDM or PTFE/FEP-encapsulated seals instead.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acrylate causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: n-Butyl Acrylate causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Acid-catalyzed esterification of acrylic acid with 1-butanol
Downstream Derivatives
  • Acrylic latex architectural paints and pressure-sensitive adhesives (PSA)
  • ASA weather-resistant engineering plastics and acrylic elastomers
Typical Industrial Uses
  • Soft-monomer building block for acrylic emulsion paints and caulks
  • Key monomer in pressure-sensitive tapes, labels, and textile binders
  • Impact modifier for ASA and PVC plastics

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source n-Butyl Acrylate & Compatible Equipment

n-Butyl Acrylate Industrial / Reagent Grade (CAS 141-32-2)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
n-Butyl Acrylate Bulk Chemical Suppliers & Packaging

Verified ISO-certified chemical manufacturers

View Suppliers on Made-in-China.com