CHEMICAL · CAS 62-53-3

Aniline

CAS 62-53-3 · EC 200-539-3 · C6H7N · UN1547

Primary aromatic amine manufactured by hydrogenating nitrobenzene, with roughly 85% consumed to produce MDI for rigid polyurethane insulation foams and adhesives.

Also known as: Phenylamine, Aminobenzene, Benzenamine

Molecular Weight
93.13 g/mol
Boiling Point
184.1 °C
Melting Point
-6 °C
Flash Point
70 °C
Density
1.0217 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Aniline chemical identifiers
Identifier Value
CAS Registry Number 62-53-3
EC Number 200-539-3
Molecular Formula C6H7N
Molecular Weight 93.13 g/mol
IUPAC Name aniline
Canonical SMILES C1=CC=C(C=C1)N
InChI InChI=1S/C6H7N/c7-6-4-2-1-3-5-6/h1-5H,7H2
InChIKey PAYRUJLWNCNPSJ-UHFFFAOYSA-N
UN Transport Number UN1547
PubChem CID 6115

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 6115

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Aniline (CAS 62-53-3) unless otherwise noted.

Density (vs. Water = 1.0)1.0217 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-6 °C
-13020 °C260
Boiling Point184.1 °C
-50Water 100 °C350
Flash Point (Closed Cup)70 °C
-50GHS Cat.2 (23 °C)220
Aniline physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless to amber oily liquid (darkens in air) with characteristic amine odor
Density 1.0217 g/cm³ (20 °C) (8.53 lb/gal)
Melting Point -6 °C (21.2 °F)
Boiling Point 184.1 °C (363.4 °F)
Flash Point 70 °C (158 °F (closed cup))
Vapor Pressure 0.49 mmHg (25 °C)
Water Solubility 36 g/L (20 °C)
pH / pKa pKa (conj. acid) 4.63
Viscosity 3.85 mPa·s (25 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS05 Corrosive
GHS06 Acute Toxicity
GHS08 Health Hazard
GHS09 Environmental
Acute Toxicity — Oral/Dermal/Inhalation (Cat. 3) · Serious Eye Damage (Cat. 1) · Carcinogenicity (Cat. 2) · STOT — Repeated Exposure (Cat. 1, methemoglobinemia)
Hazard statements
  • H301+H311+H331: Toxic if swallowed, in contact with skin or inhaled
  • H318: Causes serious eye damage
  • H351: Suspected of causing cancer
  • H372: Causes blood/organ damage
  • H400: Very toxic to aquatic life
Key precautionary statements
  • P260: Do not breathe vapors
  • P280: Wear butyl gloves, apron, and full face shield
  • P273: Avoid release to the environment

Handling & storage: Store under nitrogen in dark vessels. Aggressively attacks ABS, PC, PVC-U, PS, PMMA, PET, PBT, and NBR; restrict wetted contact to PTFE, FEP, PFA, PEEK, PPS, or EPDM.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Aniline

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Aniline
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Aniline at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Aniline at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes severe attack, swelling, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Aniline at 20 °C with negligible swelling, weight change, or mechanical degradation in PA66 (Nylon 66).
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Aniline at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes severe attack, swelling, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes severe attack, swelling, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Aniline at 20 °C with negligible swelling, weight change, or mechanical degradation in PA6 (Nylon 6).
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Aniline at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes severe attack, swelling, crazing, or rapid structural failure in PBT even under short-term contact.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes severe attack, swelling, crazing, or rapid structural failure in PET even under short-term contact.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes severe attack, swelling, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Aniline at 20 °C; moderate swelling, softening, or stress-cracking risk makes UHMWPE unsuitable for continuous containment.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes severe attack, swelling, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Aniline at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Aniline at 20 °C with negligible swelling, weight change, or mechanical degradation in PVDF.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Aniline at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Aniline at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Aniline at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Aniline at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Aniline at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes rapid swelling, softening, and seal failure in FKM (Viton) fluoroelastomer; consider EPDM or PTFE/FEP-encapsulated seals instead.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Aniline causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Catalytic hydrogenation of nitrobenzene
Downstream Derivatives
  • Methylene diphenyl diisocyanate (MDI) for rigid polyurethane foams (~85% of demand)
  • Rubber vulcanization accelerators/antioxidants and azo/indigo dyes
Typical Industrial Uses
  • Primary petrochemical precursor for MDI polyurethane insulation and adhesives
  • Feedstock for rubber tire accelerators (MBT/CBS) and antiozonants
  • Intermediate for indigo denim dye, herbicides, and paracetamol

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Aniline & Compatible Equipment

Aniline Industrial / Reagent Grade (CAS 62-53-3)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Aniline Bulk Chemical Suppliers & Packaging