Formic Acid (85%)
Simplest and strongest unsubstituted carboxylic acid, widely used in leather tanning, textile dyeing, rubber latex coagulation, descaling cleaners, and livestock silage preservation.
Also known as: Methanoic acid, Aminic acid, Hydrogen carboxylic acid
Registry Numbers & Structural Strings
| Identifier | Value |
|---|---|
| CAS Registry Number | 64-18-6 |
| EC Number | 200-579-1 |
| Molecular Formula | CH2O2 |
| Molecular Weight | 46.02 g/mol |
| IUPAC Name | formic acid |
| Canonical SMILES | C(=O)O |
| InChI | InChI=1S/CH2O2/c2-1-3/h1H,(H,2,3) |
| InChIKey | BDAGIHXWWSANSR-UHFFFAOYSA-N |
| UN Transport Number | UN1779 |
| PubChem CID | 284 |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 284
Measured Constants (SI / Imperial)
CAS identifiers refer to pure methanoic acid; density, freezing/boiling points, and compatibility ratings reflect standard 85% w/w commercial formic acid.
| Property | Value |
|---|---|
| Physical State | Liquid |
| Appearance | Colorless fuming liquid with pungent, penetrating odor |
| Density | 1.195 g/cm³ (20 °C, 85%) (9.97 lb/gal) |
| Melting Point | -13 °C (8.6 °F) |
| Boiling Point | 107.3 °C (225.1 °F) |
| Flash Point | 59 °C (138.2 °F (closed cup)) |
| Vapor Pressure | 23 mmHg (20 °C, 85%) |
| Water Solubility | Miscible in all proportions |
| pH / pKa | pKa 3.75 (25 °C) |
| Viscosity | 1.58 mPa·s (20 °C, 85%) |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
GHS Classification & Precautions
- H226: Flammable liquid and vapor
- H302: Harmful if swallowed
- H314: Causes severe skin burns and eye damage
- H331: Toxic if inhaled
- P260: Do not breathe vapors
- P280: Wear acid-resistant gloves and face shield
- P403+P233: Store in vented, cool, corrosion-resistant containers
Handling & storage: Store in vented HDPE, PP, PVDF, or PTFE containers (slowly decomposes to CO + H2O over time, building pressure). Rapidly dissolves polyamides (PA6/PA66 — formic acid is a known nylon solvent) and degrades POM.
Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25
Plastics in Contact with Formic Acid (85%)
Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.
| Plastic Family | Rating & Conditions | Engineering Notes |
|---|---|---|
| Polypropylene (PP)
ISO 1043: PP | Excellent resistance to 85% formic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed polypropylene (PP). Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C) | |
| High-Density Polyethylene (HDPE)
ISO 1043: PE-HD | Excellent resistance to 85% formic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed HDPE. Grade basis: High-density polyethylene (PE100 / blow-molding HDPE) | |
| Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS | Limited resistance to 85% formic acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes ABS unsuitable for continuous pressurized containment. Grade basis: General-purpose unreinforced ABS molding grade | |
| Polycarbonate (PC)
ISO 1043: PC | Good resistance to 85% formic acid at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Unfilled bisphenol-A polycarbonate (PC) | |
| Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66 | Severe attack: 85% formic acid is a strong solvent for polyamides and rapidly dissolves PA66 (Nylon 66). Specify PP, HDPE, PVDF, or PTFE. Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66) | |
| Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD | Excellent resistance to 85% formic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed LDPE. Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade) | |
| Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U | Limited resistance to 85% formic acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes rigid PVC (PVC-U) unsuitable for continuous pressurized containment. Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade) | |
| Polystyrene (GPPS) (PS)
ISO 1043: PS | Not recommended: 85% formic acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact. Grade basis: General-purpose crystal polystyrene (GPPS) | |
| Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6 | Severe attack: 85% formic acid is a strong solvent for polyamides and rapidly dissolves PA6 (Nylon 6). Specify PP, HDPE, PVDF, or PTFE. Grade basis: Unreinforced polyamide 6 (extruded/molded PA6) | |
| Polyoxymethylene (Acetal) (POM)
ISO 1043: POM | Excellent resistance to 85% formic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed acetal (POM). Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H) | |
| Polybutylene Terephthalate (PBT)
ISO 1043: PBT | Good resistance to 85% formic acid at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Unreinforced polybutylene terephthalate (PBT) | |
| Polyethylene Terephthalate (PET)
ISO 1043: PET | Limited resistance to 85% formic acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes PET unsuitable for continuous pressurized containment. Grade basis: Semi-crystalline / oriented PET resin | |
| Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA | Not recommended: 85% formic acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact. Grade basis: Cast & extruded polymethyl methacrylate (PMMA) | |
| Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW | Excellent resistance to 85% formic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed UHMWPE. Grade basis: Virgin compression-molded UHMWPE (>3M g/mol) | |
| Styrene-Acrylonitrile (SAN)
ISO 1043: SAN | Excellent resistance to 85% formic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed SAN. Grade basis: Transparent styrene-acrylonitrile copolymer (SAN) | |
| Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE | Good resistance to 85% formic acid at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade) | |
| Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF | Excellent resistance to 85% formic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PVDF. Grade basis: Homopolymer PVDF (pipe, valve & sheet grade) | |
| Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP | Virtually inert to 85% formic acid at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media. Grade basis: Melt-extruded FEP tubing & lining grade | |
| Polyether Ether Ketone (PEEK)
ISO 1043: PEEK | Excellent resistance to 85% formic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PEEK. Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class) | |
| Polyphenylene Sulfide (PPS)
ISO 1043: PPS | Good resistance to 85% formic acid at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Linear / 40% glass-filled PPS (PPS-GF40) | |
| Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA | Virtually inert to Formic Acid (85%) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: High-purity melt-processable PFA tubing & lining grade | |
| Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM | Good resistance to Formic Acid (85%) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A) | |
| Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM | Limited resistance to Formic Acid (85%) at 20 °C; moderate swelling, softening, or stress-cracking risk makes FKM (Viton) fluoroelastomer unsuitable for continuous containment. Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine) | |
| Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR | Not recommended: Formic Acid (85%) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact. Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N) | |
| Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ | Limited resistance to Formic Acid (85%) at 20 °C; moderate swelling, softening, or stress-cracking risk makes VMQ silicone rubber unsuitable for continuous containment. Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ) |
Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25
Upstream, Downstream & Applications
- Hydrolysis of methyl formate produced from methanol and carbon monoxide
- Livestock feed/silage preservatives and potassium formate de-icers
- Natural rubber latex coagulants and leather deliming/tanning
- Coagulant in natural rubber production and leather tanning
- Industrial descaling, boiler cleaning, and textile dyeing
- Solvent for polyamide (nylon) bonding and viscosity testing
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
Source Formic Acid (85%) & Compatible Equipment
85% w/w Aqueous Acid · Bulk drums / IBCs
View Suppliers on Made-in-China.comPP-H / HDPE / PVDF / PTFE-lined chemical tanks & valves
View Suppliers on Made-in-China.com