CHEMICAL · CAS 64-19-7

Acetic Acid (Glacial)

CAS 64-19-7 · EC 200-580-7 · C2H4O2 · UN2789

Corrosive, pungent weak carboxylic acid that is a cornerstone chemical intermediate for vinyl acetate monomer (VAM), purified terephthalic acid (PTA) for PET, and acetate esters.

Also known as: Ethanoic acid, Glacial acetic acid (GAA), Methanecarboxylic acid

Molecular Weight
60.05 g/mol
Boiling Point
117.9 °C
Melting Point
16.6 °C
Flash Point
39 °C
Density
1.0492 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Acetic Acid (Glacial) chemical identifiers
Identifier Value
CAS Registry Number 64-19-7
EC Number 200-580-7
Molecular Formula C2H4O2
Molecular Weight 60.05 g/mol
IUPAC Name acetic acid
Canonical SMILES CC(=O)O
InChI InChI=1S/C2H4O2/c1-2(3)4/h1H3,(H,3,4)
InChIKey QTBSBXVTEAMEQO-UHFFFAOYSA-N
UN Transport Number UN2789
PubChem CID 176

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 176

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Acetic Acid (Glacial) (CAS 64-19-7) unless otherwise noted.

Density (vs. Water = 1.0)1.0492 g/cm³
0.5Water 1.02.5
Melting / Freezing Point16.6 °C
-13020 °C260
Boiling Point117.9 °C
-50Water 100 °C350
Flash Point (Closed Cup)39 °C
-50GHS Cat.2 (23 °C)220
Acetic Acid (Glacial) physical and chemical properties
Property Value
Physical State Liquid
Appearance Clear, colorless liquid with sharp vinegar odor (freezes at 16.6 °C)
Density 1.0492 g/cm³ (20 °C) (8.76 lb/gal)
Melting Point 16.6 °C (61.9 °F)
Boiling Point 117.9 °C (244.2 °F)
Flash Point 39 °C (102.2 °F (closed cup))
Vapor Pressure 15.7 mmHg (25 °C)
Water Solubility Miscible in all proportions
pH / pKa pKa 4.76 (25 °C)
Viscosity 1.13 mPa·s (25 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS02 Flammable
GHS05 Corrosive
Flammable Liquids (Category 3) · Skin Corrosion (Category 1A) · Serious Eye Damage (Category 1)
Hazard statements
  • H226: Flammable liquid and vapor
  • H314: Causes severe skin burns and eye damage
Key precautionary statements
  • P210: Keep away from heat, sparks, open flames and hot surfaces
  • P280: Wear acid-resistant gloves and face shield
  • P305+P351+P338: IF IN EYES: Rinse cautiously with water

Handling & storage: Store above 18 °C to prevent freezing/expansion in lines. Glacial (100%) acetic acid attacks PA6, PA66, POM, ABS, and PMMA; specify PTFE, FEP, PVDF, PEEK, PPS, or ambient PP/HDPE.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Acetic Acid (Glacial)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Acetic Acid (Glacial)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
A Excellent 20 °C · 100% (Glacial) · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to glacial acetic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed polypropylene (PP).
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
A Excellent 20 °C · 100% (Glacial) · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to glacial acetic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed HDPE.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 100% (Glacial) · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: glacial acetic acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
C Fair 20 °C · 100% (Glacial) · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to glacial acetic acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes polycarbonate (PC) unsuitable for continuous pressurized containment.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
D Not recommended 20 °C · 100% (Glacial) · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: glacial acetic acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in PA66 (Nylon 66) even under short-term contact.
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
A Excellent 20 °C · 100% (Glacial) · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to glacial acetic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed LDPE.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
C Fair 20 °C · 100% (Glacial) · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to glacial acetic acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes rigid PVC (PVC-U) unsuitable for continuous pressurized containment.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% (Glacial) · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: glacial acetic acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
D Not recommended 20 °C · 100% (Glacial) · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: glacial acetic acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in PA6 (Nylon 6) even under short-term contact.
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
A Excellent 20 °C · 100% (Glacial) · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to glacial acetic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed acetal (POM).
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
B Good 20 °C · 100% (Glacial) · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to glacial acetic acid at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
B Good 20 °C · 100% (Glacial) · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to glacial acetic acid at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 100% (Glacial) · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: glacial acetic acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
A Excellent 20 °C · 100% (Glacial) · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to glacial acetic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed UHMWPE.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
A Excellent 20 °C · 100% (Glacial) · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to glacial acetic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed SAN.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
B Good 20 °C · 100% (Glacial) · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to glacial acetic acid at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
A Excellent 20 °C · 100% (Glacial) · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to glacial acetic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PVDF.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 100% (Glacial) · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to glacial acetic acid at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% (Glacial) · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to glacial acetic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% (Glacial) · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to glacial acetic acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% (Glacial) · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Acetic Acid (Glacial) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
B Good 20 °C · 100% (Glacial) · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Acetic Acid (Glacial) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
C Fair 20 °C · 100% (Glacial) · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Acetic Acid (Glacial) at 20 °C; moderate swelling, softening, or stress-cracking risk makes FKM (Viton) fluoroelastomer unsuitable for continuous containment.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 100% (Glacial) · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Acetic Acid (Glacial) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
C Fair 20 °C · 100% (Glacial) · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Acetic Acid (Glacial) at 20 °C; moderate swelling, softening, or stress-cracking risk makes VMQ silicone rubber unsuitable for continuous containment.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Methanol carbonylation (Monsanto / Cativa rhodium-iridium process)
Downstream Derivatives
  • Vinyl acetate monomer (VAM) for PVA/EVA adhesives
  • Solvent for terephthalic acid (PTA) oxidation in PET production
  • Ethyl acetate, butyl acetate, and acetic anhydride
Typical Industrial Uses
  • Feedstock for VAM, acetate esters, and cellulose acetate
  • Process solvent in PTA manufacturing for PET bottles/fibers
  • Textile dyeing pH buffer and printed-circuit / chemical etching

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Acetic Acid (Glacial) & Compatible Equipment

Acetic Acid Industrial / Reagent Grade (CAS 64-19-7)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Corrosion-Resistant Storage Tanks & Piping for Acetic Acid

PP-H / HDPE / PVDF / PTFE-lined chemical tanks & valves

View Suppliers on Made-in-China.com