Isopropanol (IPA)
Secondary three-carbon alcohol widely used for electronics flux removal, precision optical cleaning, pharmaceutical sanitizing, and coatings solvent blending.
Also known as: Isopropyl alcohol, Propan-2-ol, 2-Propanol, Rubbing alcohol
Registry Numbers & Structural Strings
| Identifier | Value |
|---|---|
| CAS Registry Number | 67-63-0 |
| EC Number | 200-661-7 |
| Molecular Formula | C3H8O |
| Molecular Weight | 60.1 g/mol |
| IUPAC Name | propan-2-ol |
| Canonical SMILES | CC(C)O |
| InChI | InChI=1S/C3H8O/c1-3(2)4/h3-4H,1-2H3 |
| InChIKey | KFZMGEQAYNKOFK-UHFFFAOYSA-N |
| UN Transport Number | UN1219 |
| PubChem CID | 3776 |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 3776
Measured Constants (SI / Imperial)
Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Isopropanol (IPA) (CAS 67-63-0) unless otherwise noted.
| Property | Value |
|---|---|
| Physical State | Liquid |
| Appearance | Colorless, clear liquid with sharp alcoholic odor |
| Density | 0.7855 g/cm³ (20 °C) (6.56 lb/gal) |
| Melting Point | -89 °C (-128.2 °F) |
| Boiling Point | 82.6 °C (180.7 °F) |
| Flash Point | 12 °C (53.6 °F (closed cup)) |
| Vapor Pressure | 45.4 mmHg (25 °C) |
| Water Solubility | Miscible in all proportions |
| pH / pKa | pKa 16.5 (25 °C) |
| Viscosity | 2.04 mPa·s (25 °C) |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
GHS Classification & Precautions
- H225: Highly flammable liquid and vapor
- H319: Causes serious eye irritation
- H336: May cause drowsiness or dizziness
- P210: Keep away from heat, sparks, open flames and hot surfaces
- P233: Keep container tightly closed
- P305+P351+P338: IF IN EYES: Rinse cautiously with water for several minutes
Handling & storage: Store in tightly closed containers inside flammable-liquid cabinets. Compatible with PP, HDPE, LDPE, POM, and PTFE; avoid unstressed/stressed PMMA (crazing).
Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25
Plastics in Contact with Isopropanol (IPA)
Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.
| Plastic Family | Rating & Conditions | Engineering Notes |
|---|---|---|
| Polypropylene (PP)
ISO 1043: PP | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed polypropylene (PP). Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C) | |
| High-Density Polyethylene (HDPE)
ISO 1043: PE-HD | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed HDPE. Grade basis: High-density polyethylene (PE100 / blow-molding HDPE) | |
| Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS | Good resistance to isopropanol (IPA) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: General-purpose unreinforced ABS molding grade | |
| Polycarbonate (PC)
ISO 1043: PC | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed polycarbonate (PC). Grade basis: Unfilled bisphenol-A polycarbonate (PC) | |
| Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66 | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA66 (Nylon 66). Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66) | |
| Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed LDPE. Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade) | |
| Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed rigid PVC (PVC-U). Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade) | |
| Polystyrene (GPPS) (PS)
ISO 1043: PS | Good resistance to isopropanol (IPA) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: General-purpose crystal polystyrene (GPPS) | |
| Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6 | Good resistance to isopropanol (IPA) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Unreinforced polyamide 6 (extruded/molded PA6) | |
| Polyoxymethylene (Acetal) (POM)
ISO 1043: POM | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed acetal (POM). Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H) | |
| Polybutylene Terephthalate (PBT)
ISO 1043: PBT | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PBT. Grade basis: Unreinforced polybutylene terephthalate (PBT) | |
| Polyethylene Terephthalate (PET)
ISO 1043: PET | Good resistance to isopropanol (IPA) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Semi-crystalline / oriented PET resin | |
| Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA | Not recommended: isopropanol (IPA) causes severe chemical attack, dissolution, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact. Grade basis: Cast & extruded polymethyl methacrylate (PMMA) | |
| Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed UHMWPE. Grade basis: Virgin compression-molded UHMWPE (>3M g/mol) | |
| Styrene-Acrylonitrile (SAN)
ISO 1043: SAN | Good resistance to isopropanol (IPA) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature. Grade basis: Transparent styrene-acrylonitrile copolymer (SAN) | |
| Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE | Virtually inert to isopropanol (IPA) at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media. Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade) | |
| Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PVDF. Grade basis: Homopolymer PVDF (pipe, valve & sheet grade) | |
| Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP | Virtually inert to isopropanol (IPA) at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media. Grade basis: Melt-extruded FEP tubing & lining grade | |
| Polyether Ether Ketone (PEEK)
ISO 1043: PEEK | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PEEK. Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class) | |
| Polyphenylene Sulfide (PPS)
ISO 1043: PPS | Excellent resistance to isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PPS. Grade basis: Linear / 40% glass-filled PPS (PPS-GF40) | |
| Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA | Virtually inert to Isopropanol (IPA) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: High-purity melt-processable PFA tubing & lining grade | |
| Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM | Excellent resistance to Isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical degradation in EPDM rubber. Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A) | |
| Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM | Excellent resistance to Isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer. Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine) | |
| Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR | Good resistance to Isopropanol (IPA) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N) | |
| Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ | Excellent resistance to Isopropanol (IPA) at 20 °C with negligible swelling, weight change, or mechanical degradation in VMQ silicone rubber. Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ) |
Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25
Upstream, Downstream & Applications
- Direct or indirect catalytic hydration of propylene
- Catalytic hydrogenation of acetone
- Acetone via catalytic dehydrogenation
- Isopropyl acetate and isopropyl amines
- Semiconductor-grade cleaning formulations
- Electronics PCB defluxing and semiconductor wafer drying
- Industrial disinfectant and pharmaceutical extraction solvent
- Coatings, inks, and de-icing fluid formulations
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
Source Isopropanol (IPA) & Compatible Equipment
High-purity industrial grade · Bulk supply
View Suppliers on Made-in-China.comHDPE / PTFE / FKM / EPDM solvent transfer equipment
View Suppliers on Made-in-China.com