CHEMICAL · CAS 75-09-2

Dichloromethane (DCM)

CAS 75-09-2 · EC 200-838-9 · CH2Cl2 · UN1593

Dense, non-flammable, ultra-volatile chlorinated solvent with extreme solvency power used for acrylic/polycarbonate solvent welding, paint stripping, polyurethane foam blowing, and pharmaceutical extraction.

Also known as: Methylene chloride, Methylene dichloride, R-30

Molecular Weight
84.93 g/mol
Boiling Point
39.6 °C
Melting Point
-96.7 °C
Flash Point
—
Density
1.3266 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Dichloromethane (DCM) chemical identifiers
Identifier Value
CAS Registry Number 75-09-2
EC Number 200-838-9
Molecular Formula CH2Cl2
Molecular Weight 84.93 g/mol
IUPAC Name dichloromethane
Canonical SMILES C(Cl)Cl
InChI InChI=1S/CH2Cl2/c2-1-3/h1H2
InChIKey YMWUJEATGCHHMB-UHFFFAOYSA-N
UN Transport Number UN1593
PubChem CID 6344

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 6344

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Dichloromethane (DCM) (CAS 75-09-2) unless otherwise noted.

Density (vs. Water = 1.0)1.3266 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-96.7 °C
-13020 °C260
Boiling Point39.6 °C
-50Water 100 °C350
Dichloromethane (DCM) physical and chemical properties
Property Value
Physical State Liquid
Appearance Clear, colorless heavy volatile liquid with sweet chloroform-like odor
Density 1.3266 g/cm³ (20 °C) (11.07 lb/gal)
Melting Point -96.7 °C (-142.1 °F)
Boiling Point 39.6 °C (103.3 °F)
Flash Point —
Vapor Pressure 435 mmHg (25 °C)
Water Solubility 13.2 g/L (25 °C)
pH / pKa Neutral (non-ionizable)
Viscosity 0.413 mPa·s (25 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS08 Health Hazard
GHS07 Irritant / Harmful
Carcinogenicity (Category 2) · Skin & Eye Irritation (Category 2) · STOT — Single Exposure (Category 3, CNS/carboxyhemoglobin)
Hazard statements
  • H315: Causes skin irritation
  • H319: Causes serious eye irritation
  • H336: May cause drowsiness or dizziness
  • H351: Suspected of causing cancer
Key precautionary statements
  • P261: Avoid breathing vapors
  • P280: Wear PVA/Viton chemical gloves and eye protection
  • P271: Use only in well-ventilated fume hoods

Handling & storage: Store in cool, shaded containers below 25 °C due to low boiling point (39.6 °C). Rapidly dissolves PC, PMMA, ABS, PS, SAN, and attacks PVC, PBT, and PA6; restrict contact to PTFE, FEP, PEEK, PPS, or glass.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Dichloromethane (DCM)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Dichloromethane (DCM)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to dichloromethane (DCM) at 20 °C; moderate swelling, softening, or stress-cracking risk makes polypropylene (PP) unsuitable for continuous pressurized containment.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to dichloromethane (DCM) at 20 °C; moderate swelling, softening, or stress-cracking risk makes HDPE unsuitable for continuous pressurized containment.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: dichloromethane (DCM) causes severe chemical attack, dissolution, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: dichloromethane (DCM) causes severe chemical attack, dissolution, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to dichloromethane (DCM) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PA66 (Nylon 66) unsuitable for continuous pressurized containment.
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: dichloromethane (DCM) causes severe chemical attack, dissolution, crazing, or rapid structural failure in LDPE even under short-term contact.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: dichloromethane (DCM) causes severe chemical attack, dissolution, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: dichloromethane (DCM) causes severe chemical attack, dissolution, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to dichloromethane (DCM) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PA6 (Nylon 6) unsuitable for continuous pressurized containment.
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: dichloromethane (DCM) causes severe chemical attack, dissolution, crazing, or rapid structural failure in acetal (POM) even under short-term contact.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: dichloromethane (DCM) causes severe chemical attack, dissolution, crazing, or rapid structural failure in PBT even under short-term contact.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: dichloromethane (DCM) causes severe chemical attack, dissolution, crazing, or rapid structural failure in PET even under short-term contact.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: dichloromethane (DCM) causes severe chemical attack, dissolution, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to dichloromethane (DCM) at 20 °C; moderate swelling, softening, or stress-cracking risk makes UHMWPE unsuitable for continuous pressurized containment.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: dichloromethane (DCM) causes severe chemical attack, dissolution, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to dichloromethane (DCM) at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to dichloromethane (DCM) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PVDF.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to dichloromethane (DCM) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to dichloromethane (DCM) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to dichloromethane (DCM) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Dichloromethane (DCM) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Dichloromethane (DCM) severely swells and degrades EPDM rubber; specify FKM (Viton) or PTFE/PFA seals for hydrocarbon or strong-acid service.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Dichloromethane (DCM) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Dichloromethane (DCM) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Dichloromethane (DCM) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Direct chlorination of methane or methyl chloride
Downstream Derivatives
  • Pharmaceutical API extraction and polycarbonate interfacial polymerization
  • Acrylic/PC solvent welding adhesives and paint removers
Typical Industrial Uses
  • Process solvent for polycarbonate (PC) polymerization and film casting
  • Solvent welding of PMMA (acrylic) and PC parts
  • Pharmaceutical synthesis, metal degreasing, and chemical extraction

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Dichloromethane (DCM) & Compatible Equipment

Dichloromethane Industrial / Reagent Grade (CAS 75-09-2)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Solvent-Resistant Chemical Drums, Pumps & Seals

HDPE / PTFE / FKM / EPDM solvent transfer equipment

View Suppliers on Made-in-China.com