Perchloric Acid (70%)
Super-strong oxidizing mineral acid used in analytical metallurgy digestion, metal electropolishing, and flat-panel display chrome etching, requiring fluoropolymer containment.
Also known as: Hyperchloric acid, HClO4
Registry Numbers & Structural Strings
| Identifier | Value |
|---|---|
| CAS Registry Number | 7601-90-3 |
| EC Number | 231-512-4 |
| Molecular Formula | ClHO4 |
| Molecular Weight | 100.46 g/mol |
| IUPAC Name | perchloric acid |
| Canonical SMILES | OCl(=O)(=O)=O |
| InChI | InChI=1S/ClHO4/c2-1(3,4)5/h(H,2,3,4,5) |
| InChIKey | VLTRZXGMWDSKGL-UHFFFAOYSA-N |
| UN Transport Number | UN1873 |
| PubChem CID | 24247 |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 24247
Measured Constants (SI / Imperial)
CAS identifiers refer to anhydrous HClO4; physical properties and compatibility ratings reflect standard 70% w/w aqueous perchloric acid.
| Property | Value |
|---|---|
| Physical State | Liquid (70% aq.) |
| Appearance | Clear, colorless odorless dense aqueous liquid |
| Density | 1.67 g/cm³ (20 °C, 70%) (13.94 lb/gal) |
| Melting Point | -18 °C (-0.4 °F) |
| Boiling Point | 203 °C (397.4 °F) |
| Flash Point | — |
| Vapor Pressure | 6.8 mmHg (25 °C) |
| Water Solubility | Miscible in all proportions |
| pH / pKa | pKa ~-10 (superacid) |
| Viscosity | 3.6 mPa·s (20 °C) |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
GHS Classification & Precautions
- H271: May cause fire or explosion; strong oxidizer
- H290: May be corrosive to metals
- H314: Causes severe skin burns and eye damage
- P220: Keep strictly segregated from organics, wood, and combustibles
- P280: Use dedicated wash-down perchloric fume hood and acid PPE
Handling & storage: Handle only in dedicated wash-down fume hoods (anhydrous perchlorate salts are shock-explosive). Restrict wetted plastics to PTFE, FEP, PFA, or PVDF; avoid PA6/PA66, POM, ABS, PC, PEEK, and PPS.
Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25
Plastics in Contact with Perchloric Acid (70%)
Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.
| Plastic Family | Rating & Conditions | Engineering Notes |
|---|---|---|
| Polypropylene (PP)
ISO 1043: PP | Good resistance to Perchloric Acid (70%) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C) | |
| High-Density Polyethylene (HDPE)
ISO 1043: PE-HD | Good resistance to Perchloric Acid (70%) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: High-density polyethylene (PE100 / blow-molding HDPE) | |
| Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in ABS even under short-term contact. Grade basis: General-purpose unreinforced ABS molding grade | |
| Polycarbonate (PC)
ISO 1043: PC | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact. Grade basis: Unfilled bisphenol-A polycarbonate (PC) | |
| Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66 | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in PA66 (Nylon 66) even under short-term contact. Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66) | |
| Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD | Limited resistance to Perchloric Acid (70%) at 20 °C; moderate swelling, softening, or stress-cracking risk makes LDPE unsuitable for continuous containment. Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade) | |
| Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact. Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade) | |
| Polystyrene (GPPS) (PS)
ISO 1043: PS | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact. Grade basis: General-purpose crystal polystyrene (GPPS) | |
| Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6 | Limited resistance to Perchloric Acid (70%) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PA6 (Nylon 6) unsuitable for continuous containment. Grade basis: Unreinforced polyamide 6 (extruded/molded PA6) | |
| Polyoxymethylene (Acetal) (POM)
ISO 1043: POM | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in acetal (POM) even under short-term contact. Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H) | |
| Polybutylene Terephthalate (PBT)
ISO 1043: PBT | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in PBT even under short-term contact. Grade basis: Unreinforced polybutylene terephthalate (PBT) | |
| Polyethylene Terephthalate (PET)
ISO 1043: PET | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in PET even under short-term contact. Grade basis: Semi-crystalline / oriented PET resin | |
| Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact. Grade basis: Cast & extruded polymethyl methacrylate (PMMA) | |
| Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW | Limited resistance to Perchloric Acid (70%) at 20 °C; moderate swelling, softening, or stress-cracking risk makes UHMWPE unsuitable for continuous containment. Grade basis: Virgin compression-molded UHMWPE (>3M g/mol) | |
| Styrene-Acrylonitrile (SAN)
ISO 1043: SAN | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in SAN even under short-term contact. Grade basis: Transparent styrene-acrylonitrile copolymer (SAN) | |
| Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE | Virtually inert to Perchloric Acid (70%) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade) | |
| Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF | Excellent resistance to Perchloric Acid (70%) at 20 °C with negligible swelling, weight change, or mechanical degradation in PVDF. Grade basis: Homopolymer PVDF (pipe, valve & sheet grade) | |
| Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP | Good resistance to Perchloric Acid (70%) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Melt-extruded FEP tubing & lining grade | |
| Polyether Ether Ketone (PEEK)
ISO 1043: PEEK | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in PEEK even under short-term contact. Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class) | |
| Polyphenylene Sulfide (PPS)
ISO 1043: PPS | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in PPS even under short-term contact. Grade basis: Linear / 40% glass-filled PPS (PPS-GF40) | |
| Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA | Virtually inert to Perchloric Acid (70%) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: High-purity melt-processable PFA tubing & lining grade | |
| Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM | Limited resistance to Perchloric Acid (70%) at 20 °C; moderate swelling, softening, or stress-cracking risk makes EPDM rubber unsuitable for continuous containment. Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A) | |
| Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM | Excellent resistance to Perchloric Acid (70%) at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer. Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine) | |
| Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact. Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N) | |
| Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ | Not recommended: Perchloric Acid (70%) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact. Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ) |
Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25
Upstream, Downstream & Applications
- Anodic oxidation of aqueous sodium chlorate followed by acidification/distillation
- Analytical wet digestion of ores/alloys and electropolishing of metals
- Ammonium perchlorate solid rocket propellants and LCD chromium etchant
- Analytical chemistry acid digestion and metal electropolishing
- Chrome etching in flat-panel display (LCD) lithography
- Precursor for ammonium perchlorate oxidizers
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
Source Perchloric Acid (70%) & Compatible Equipment
70% w/w Aqueous Acid · Bulk drums / IBCs
View Suppliers on Made-in-China.comPP-H / HDPE / PVDF / PTFE-lined chemical tanks & valves