CHEMICAL · CAS 7664-39-3

Hydrofluoric Acid (48% HF)

CAS 7664-39-3 · EC 231-634-8 · FH · UN1790

Extremely hazardous, glass-dissolving mineral acid that is the indispensable fluorine feedstock for all fluoropolymers (PTFE/PVDF/PFA/FKM) and semiconductor silicon etching.

Also known as: Hydrogen fluoride solution, Fluoric acid, HF

Molecular Weight
20.01 g/mol
Boiling Point
108 °C
Melting Point
-35 °C
Flash Point
—
Density
1.15 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Hydrofluoric Acid (48% HF) chemical identifiers
Identifier Value
CAS Registry Number 7664-39-3
EC Number 231-634-8
Molecular Formula FH
Molecular Weight 20.01 g/mol
IUPAC Name fluorane
Canonical SMILES F
InChI InChI=1S/FH/h1H
InChIKey KRHYYFGTRYWZRS-UHFFFAOYSA-N
UN Transport Number UN1790
PubChem CID 14917

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 14917

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Solution Basis · 48% w/w Aqueous Acid MEASUREMENT BASIS

CAS identifiers refer to anhydrous HF; physical properties and compatibility ratings reflect standard 48% w/w reagent-grade aqueous hydrofluoric acid.

Density (vs. Water = 1.0)1.15 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-35 °C
-13020 °C260
Boiling Point108 °C
-50Water 100 °C350
Hydrofluoric Acid (48% HF) physical and chemical properties
Property Value
Physical State Liquid (48% aq.)
Appearance Colorless fuming aqueous liquid with sharp penetrating odor
Density 1.15 g/cm³ (20 °C, 48%) (9.60 lb/gal)
Melting Point -35 °C (-31 °F)
Boiling Point 108 °C (226.4 °F)
Flash Point —
Vapor Pressure 25 mmHg (20 °C, 48%)
Water Solubility Miscible in all proportions
pH / pKa pKa 3.17 (weak acid, extreme toxicity)
Viscosity 1.1 mPa·s (20 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS05 Corrosive
GHS06 Acute Toxicity
Acute Toxicity — Oral/Dermal/Inhalation (Cat. 1–2, fatal) · Skin Corrosion (Cat. 1A, deep systemic calcium depletion)
Hazard statements
  • H300+H310+H330: Fatal if swallowed, in contact with skin or if inhaled
  • H314: Causes severe skin burns and deep tissue/bone damage
Key precautionary statements
  • P260: Do not breathe fumes
  • P280: Wear neoprene/butyl HF-rated PPE and keep calcium gluconate gel immediately on hand

Handling & storage: NEVER store in glass or ceramic (HF rapidly dissolves silica/glass). Use exclusively HDPE, PP, LDPE, PVDF, PTFE, FEP, or PFA; strictly avoid PA6/PA66, POM, PC, and glass-filled plastics.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Hydrofluoric Acid (48% HF)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Hydrofluoric Acid (48% HF)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C with negligible swelling, weight change, or mechanical degradation in polypropylene (PP).
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C with negligible swelling, weight change, or mechanical degradation in HDPE.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
C Fair 20 °C · 48% aq. · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Hydrofluoric Acid (48% HF) at 20 °C; moderate swelling, softening, or stress-cracking risk makes ABS unsuitable for continuous containment.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 48% aq. · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Hydrofluoric Acid (48% HF) causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
D Not recommended 20 °C · 48% aq. · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Hydrofluoric Acid (48% HF) causes severe attack, swelling, crazing, or rapid structural failure in PA66 (Nylon 66) even under short-term contact.
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C with negligible swelling, weight change, or mechanical degradation in LDPE.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C with negligible swelling, weight change, or mechanical degradation in rigid PVC (PVC-U).
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
B Good 20 °C · 48% aq. · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Hydrofluoric Acid (48% HF) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
D Not recommended 20 °C · 48% aq. · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Hydrofluoric Acid (48% HF) causes severe attack, swelling, crazing, or rapid structural failure in PA6 (Nylon 6) even under short-term contact.
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
D Not recommended 20 °C · 48% aq. · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Hydrofluoric Acid (48% HF) causes severe attack, swelling, crazing, or rapid structural failure in acetal (POM) even under short-term contact.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
C Fair 20 °C · 48% aq. · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Hydrofluoric Acid (48% HF) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PBT unsuitable for continuous containment.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
C Fair 20 °C · 48% aq. · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to Hydrofluoric Acid (48% HF) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PET unsuitable for continuous containment.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
B Good 20 °C · 48% aq. · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Hydrofluoric Acid (48% HF) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C with negligible swelling, weight change, or mechanical degradation in UHMWPE.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C with negligible swelling, weight change, or mechanical degradation in SAN.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
B Good 20 °C · 48% aq. · Ambient contact
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C; fluoropolymers are the mandatory industrial standard for hydrofluoric acid containment (glass is rapidly dissolved).
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C; fluoropolymers are the mandatory industrial standard for hydrofluoric acid containment (glass is rapidly dissolved).
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C; fluoropolymers are the mandatory industrial standard for hydrofluoric acid containment (glass is rapidly dissolved).
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C; fluoropolymers are the mandatory industrial standard for hydrofluoric acid containment (glass is rapidly dissolved).
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
B Good 20 °C · 48% aq. · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to Hydrofluoric Acid (48% HF) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
A Excellent 20 °C · 48% aq. · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Hydrofluoric Acid (48% HF) at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 48% aq. · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Hydrofluoric Acid (48% HF) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 48% aq. · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Hydrofluoric Acid (48% HF) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Reaction of fluorspar (CaF2) with concentrated sulfuric acid
Downstream Derivatives
  • Fluoropolymers (PTFE, PVDF, FEP, PFA, FKM) and HFC/HFO refrigerants
  • Semiconductor silicon dioxide wafer etching and stainless-steel pickling
Typical Industrial Uses
  • Foundational fluorine source for PTFE, PVDF, FEP, PFA, and FKM fluoropolymers
  • Semiconductor SiO2 wet etching and solar-cell texturing
  • Stainless-steel pickling, petroleum alkylation, and glass frosting

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Hydrofluoric Acid (48% HF) & Compatible Equipment

Hydrofluoric Acid Industrial / Reagent Grade (CAS 7664-39-3)

48% w/w Aqueous Acid · Bulk drums / IBCs

View Suppliers on Made-in-China.com
Corrosion-Resistant Storage Tanks & Piping for Hydrofluoric Acid

PP-H / HDPE / PVDF / PTFE-lined chemical tanks & valves

View Suppliers on Made-in-China.com