CHEMICAL · CAS 7664-93-9

Sulfuric Acid (98%)

CAS 7664-93-9 · EC 231-639-5 · H2O4S · UN1830

Highest-volume industrial chemical worldwide: a dense, strongly dehydrating, oxidizing mineral acid used in fertilizer production, metal pickling, chemical synthesis, and pH neutralization.

Also known as: Oil of vitriol, Dihydrogen sulfate, Battery acid (dilute)

Molecular Weight
98.08 g/mol
Boiling Point
337 °C
Melting Point
10.3 °C
Flash Point
—
Density
1.835 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Sulfuric Acid (98%) chemical identifiers
Identifier Value
CAS Registry Number 7664-93-9
EC Number 231-639-5
Molecular Formula H2O4S
Molecular Weight 98.08 g/mol
IUPAC Name sulfuric acid
Canonical SMILES OS(=O)(=O)O
InChI InChI=1S/H2O4S/c1-5(2,3)4/h(H2,1,2,3,4)
InChIKey QAOWNCQODCNURD-UHFFFAOYSA-N
UN Transport Number UN1830
PubChem CID 1118

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 1118

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Solution Basis · 98% w/w Concentrated Acid MEASUREMENT BASIS

CAS identifiers refer to pure H2SO4; density, viscosity, and compatibility ratings reflect standard 98% w/w commercial concentrated sulfuric acid.

Density (vs. Water = 1.0)1.835 g/cm³
0.5Water 1.02.5
Melting / Freezing Point10.3 °C
-13020 °C260
Boiling Point337 °C
-50Water 100 °C350
Sulfuric Acid (98%) physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless to slightly amber dense oily liquid
Density 1.835 g/cm³ (20 °C, 98%) (15.31 lb/gal)
Melting Point 10.3 °C (50.5 °F)
Boiling Point 337 °C (638.6 °F)
Flash Point —
Vapor Pressure <0.001 mmHg (25 °C)
Water Solubility Miscible with violent exotherm (always add acid to water)
pH / pKa pKa1 -3.0, pKa2 1.99
Viscosity 24.2 mPa·s (25 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS05 Corrosive
Corrosive to Metals (Category 1) · Skin Corrosion (Category 1A) · Serious Eye Damage (Category 1)
Hazard statements
  • H290: May be corrosive to metals
  • H314: Causes severe skin burns and eye damage
Key precautionary statements
  • P260: Do not breathe mist or vapors
  • P280: Wear acid-resistant gloves, apron, and full face shield
  • P305+P351+P338: IF IN EYES: Rinse cautiously with water and seek immediate medical help

Handling & storage: Store in PTFE/FEP-lined steel or high-grade PVDF/CPVC systems for 98% acid (note: concentrated 98% H2SO4 chars polyamides, POM, PEEK, and gradually attacks PP/HDPE/PVC above ambient). Never add water directly to concentrated acid.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Sulfuric Acid (98%)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Sulfuric Acid (98%)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
C Fair 20 °C · 98% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to 98% sulfuric acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes polypropylene (PP) unsuitable for continuous pressurized containment.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
C Fair 20 °C · 98% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to 98% sulfuric acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes HDPE unsuitable for continuous pressurized containment.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 98% sulfuric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 98% sulfuric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 98% sulfuric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in PA66 (Nylon 66) even under short-term contact.
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
C Fair 20 °C · 98% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to 98% sulfuric acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes LDPE unsuitable for continuous pressurized containment.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 98% sulfuric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 98% sulfuric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
C Fair 20 °C · 98% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to 98% sulfuric acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes PA6 (Nylon 6) unsuitable for continuous pressurized containment.
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 98% sulfuric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in acetal (POM) even under short-term contact.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 98% sulfuric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in PBT even under short-term contact.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 98% sulfuric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in PET even under short-term contact.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 98% sulfuric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
C Fair 20 °C · 98% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to 98% sulfuric acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes UHMWPE unsuitable for continuous pressurized containment.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 98% sulfuric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 98% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to 98% sulfuric acid at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
B Good 20 °C · 98% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to 98% sulfuric acid at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 98% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to 98% sulfuric acid at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Severe attack: concentrated 98% sulfuric acid sulfonates and dissolves PEEK at ambient temperature. Use PTFE or FEP for 98% H2SO4 service.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
B Good 20 °C · 98% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to 98% sulfuric acid at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 98% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Sulfuric Acid (98%) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Sulfuric Acid (98%) severely swells and degrades EPDM rubber; specify FKM (Viton) or PTFE/PFA seals for hydrocarbon or strong-acid service.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
A Excellent 20 °C · 98% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Sulfuric Acid (98%) at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Sulfuric Acid (98%) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 98% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Sulfuric Acid (98%) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Contact process oxidation of elemental sulfur / smelter SO2 to SO3 and absorption
Downstream Derivatives
  • Phosphoric acid and phosphate fertilizers
  • Titanium dioxide pigment, caprolactam, and metal pickling
  • Lead-acid battery electrolyte (30–38% aqueous)
Typical Industrial Uses
  • Chemical processing, sulfonation, nitration, and dehydration reagent
  • Steel pickling, ore leaching, and wastewater pH control
  • Electrolyte in automotive and industrial lead-acid batteries

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Sulfuric Acid (98%) & Compatible Equipment

Sulfuric Acid Industrial / Reagent Grade (CAS 7664-93-9)

98% w/w Concentrated Acid · Bulk drums / IBCs

View Suppliers on Made-in-China.com
Corrosion-Resistant Storage Tanks & Piping for Sulfuric Acid

PP-H / HDPE / PVDF / PTFE-lined chemical tanks & valves

View Suppliers on Made-in-China.com