CHEMICAL · CAS 7697-37-2

Nitric Acid (65%)

CAS 7697-37-2 · EC 231-714-2 · HNO3 · UN2031

Powerful, corrosive oxidizing mineral acid widely used in stainless-steel passivation, semiconductor etching, polyurethane (TDI/MDI) nitration, and ammonium nitrate fertilizer production.

Also known as: Aqua fortis, Azotic acid, Hydrogen nitrate

Molecular Weight
63.01 g/mol
Boiling Point
120.5 °C
Melting Point
-32 °C
Flash Point
—
Density
1.391 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Nitric Acid (65%) chemical identifiers
Identifier Value
CAS Registry Number 7697-37-2
EC Number 231-714-2
Molecular Formula HNO3
Molecular Weight 63.01 g/mol
IUPAC Name nitric acid
Canonical SMILES [N+](=O)(O)[O-]
InChI InChI=1S/HNO3/c2-1(3)4/h(H,2,3,4)
InChIKey GRYLNZFGIOXLOG-UHFFFAOYSA-N
UN Transport Number UN2031
PubChem CID 944

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 944

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Solution Basis · 65% w/w Aqueous Azeotrope MEASUREMENT BASIS

CAS identifiers refer to pure HNO3; physical properties and compatibility ratings reflect standard 65% w/w commercial nitric acid solution.

Density (vs. Water = 1.0)1.391 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-32 °C
-13020 °C260
Boiling Point120.5 °C
-50Water 100 °C350
Nitric Acid (65%) physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless to pale yellow fuming liquid with sharp acrid odor
Density 1.391 g/cm³ (20 °C, 65%) (11.61 lb/gal)
Melting Point -32 °C (-25.6 °F)
Boiling Point 120.5 °C (248.9 °F)
Flash Point —
Vapor Pressure 6.8 mmHg (20 °C, 65% azeotrope)
Water Solubility Miscible in all proportions
pH / pKa pKa -1.4 (strong acid)
Viscosity 1.99 mPa·s (20 °C, 65%)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS03 Oxidizer
GHS05 Corrosive
GHS06 Acute Toxicity
Oxidizing Liquids (Category 3) · Corrosive to Metals (Category 1) · Skin Corrosion (Category 1A) · Acute Toxicity — Inhalation (Category 3)
Hazard statements
  • H272: May intensify fire; oxidizer
  • H290: May be corrosive to metals
  • H314: Causes severe skin burns and eye damage
  • H331: Toxic if inhaled
Key precautionary statements
  • P220: Keep away from clothing, organics, and combustible materials
  • P260: Do not breathe fumes/vapors
  • P280: Wear acid/oxidizer-rated PPE and face shield

Handling & storage: Store in cool, vented, dark areas segregated from organics and alkalis. Strong oxidizer: 65% nitric acid rapidly degrades PA6/PA66, POM, ABS, PC, PEEK, PPS, and slowly embrittles PP/HDPE; specify PTFE, FEP, or PVDF.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Nitric Acid (65%)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Nitric Acid (65%)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
C Fair 20 °C · 65% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to 65% nitric acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes polypropylene (PP) unsuitable for continuous pressurized containment.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
C Fair 20 °C · 65% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to 65% nitric acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes HDPE unsuitable for continuous pressurized containment.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 65% nitric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 65% nitric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 65% nitric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in PA66 (Nylon 66) even under short-term contact.
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
C Fair 20 °C · 65% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to 65% nitric acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes LDPE unsuitable for continuous pressurized containment.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 65% nitric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 65% nitric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
C Fair 20 °C · 65% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to 65% nitric acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes PA6 (Nylon 6) unsuitable for continuous pressurized containment.
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 65% nitric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in acetal (POM) even under short-term contact.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 65% nitric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in PBT even under short-term contact.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 65% nitric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in PET even under short-term contact.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 65% nitric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
C Fair 20 °C · 65% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to 65% nitric acid at 20 °C; moderate swelling, softening, or stress-cracking risk makes UHMWPE unsuitable for continuous pressurized containment.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: 65% nitric acid causes severe chemical attack, dissolution, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 65% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to 65% nitric acid at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
A Excellent 20 °C · 65% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to 65% nitric acid at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PVDF.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 65% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to 65% nitric acid at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Severe oxidative degradation: concentrated 65% nitric acid attacks PEEK. Restrict wetted components to fluoropolymers (PTFE, FEP, PVDF).
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Severe oxidative degradation: concentrated 65% nitric acid attacks PPS. Restrict wetted components to fluoropolymers (PTFE, FEP, PVDF).
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 65% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Nitric Acid (65%) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Nitric Acid (65%) severely swells and degrades EPDM rubber; specify FKM (Viton) or PTFE/PFA seals for hydrocarbon or strong-acid service.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
A Excellent 20 °C · 65% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Nitric Acid (65%) at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Nitric Acid (65%) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 65% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Nitric Acid (65%) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Ostwald process catalytic oxidation of ammonia over platinum-rhodium gauze
Downstream Derivatives
  • Ammonium nitrate fertilizers and mining explosives
  • Nitrobenzene / aniline for MDI polyurethanes and adipic acid for PA66
  • Stainless steel pickling and semiconductor wet-etch blends
Typical Industrial Uses
  • Stainless steel passivation and bright-dipping baths
  • Aromatic nitration for MDI/TDI polyurethane intermediates
  • Semiconductor wafer etching and analytical digestion

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Nitric Acid (65%) & Compatible Equipment

Nitric Acid Industrial / Reagent Grade (CAS 7697-37-2)

65% w/w Aqueous Azeotrope · Bulk drums / IBCs

View Suppliers on Made-in-China.com
Corrosion-Resistant Storage Tanks & Piping for Nitric Acid

PP-H / HDPE / PVDF / PTFE-lined chemical tanks & valves

View Suppliers on Made-in-China.com