CHEMICAL · CAS 78-93-3

Methyl Ethyl Ketone (MEK)

CAS 78-93-3 · EC 201-159-0 · C4H8O · UN1193

Fast-evaporating industrial ketone solvent with high solvency power for vinyl, acrylic, polyurethane, and nitrocellulose resins, widely used in adhesives, printing inks, and PVC solvent welding.

Also known as: Butan-2-one, 2-Butanone, Ethyl methyl ketone

Molecular Weight
72.11 g/mol
Boiling Point
79.6 °C
Melting Point
-86.6 °C
Flash Point
-9 °C
Density
0.8050 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

Methyl Ethyl Ketone (MEK) chemical identifiers
Identifier Value
CAS Registry Number 78-93-3
EC Number 201-159-0
Molecular Formula C4H8O
Molecular Weight 72.11 g/mol
IUPAC Name butan-2-one
Canonical SMILES CCC(=O)C
InChI InChI=1S/C4H8O/c1-3-4(2)5/h3H2,1-2H3
InChIKey ZWEHNKRNPOVVGH-UHFFFAOYSA-N
UN Transport Number UN1193
PubChem CID 6569

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 6569

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Methyl Ethyl Ketone (MEK) (CAS 78-93-3) unless otherwise noted.

Density (vs. Water = 1.0)0.805 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-86.6 °C
-13020 °C260
Boiling Point79.6 °C
-50Water 100 °C350
Flash Point (Closed Cup)-9 °C
-50GHS Cat.2 (23 °C)220
Methyl Ethyl Ketone (MEK) physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless volatile liquid with sharp acetone-like odor
Density 0.8050 g/cm³ (20 °C) (6.72 lb/gal)
Melting Point -86.6 °C (-123.9 °F)
Boiling Point 79.6 °C (175.3 °F)
Flash Point -9 °C (15.8 °F (closed cup))
Vapor Pressure 90.6 mmHg (25 °C)
Water Solubility 275 g/L (20 °C)
pH / pKa pKa 14.7 (25 °C)
Viscosity 0.405 mPa·s (25 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS02 Flammable
GHS07 Irritant / Harmful
Flammable Liquids (Category 2) · Serious Eye Irritation (Category 2A) · STOT — Single Exposure (Category 3, narcotic effects)
Hazard statements
  • H225: Highly flammable liquid and vapor
  • H319: Causes serious eye irritation
  • H336: May cause drowsiness or dizziness
Key precautionary statements
  • P210: Keep away from heat, sparks, open flames and hot surfaces
  • P233: Keep container tightly closed
  • P240: Ground and bond container and receiving equipment

Handling & storage: Store in grounded flammable storage. Rapidly dissolves amorphous polymers (PVC-U, ABS, PC, PS, PMMA, SAN); use PTFE, FEP, PEEK, PPS, or ambient PP/HDPE.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with Methyl Ethyl Ketone (MEK)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with Methyl Ethyl Ketone (MEK)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to methyl ethyl ketone (MEK) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to methyl ethyl ketone (MEK) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: methyl ethyl ketone (MEK) causes severe chemical attack, dissolution, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: methyl ethyl ketone (MEK) causes severe chemical attack, dissolution, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to methyl ethyl ketone (MEK) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA66 (Nylon 66).
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to methyl ethyl ketone (MEK) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: methyl ethyl ketone (MEK) causes severe chemical attack, dissolution, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: methyl ethyl ketone (MEK) causes severe chemical attack, dissolution, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to methyl ethyl ketone (MEK) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA6 (Nylon 6).
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to methyl ethyl ketone (MEK) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to methyl ethyl ketone (MEK) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PBT unsuitable for continuous pressurized containment.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to methyl ethyl ketone (MEK) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PET unsuitable for continuous pressurized containment.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: methyl ethyl ketone (MEK) causes severe chemical attack, dissolution, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to methyl ethyl ketone (MEK) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: methyl ethyl ketone (MEK) causes severe chemical attack, dissolution, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to methyl ethyl ketone (MEK) at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
C Fair 20 °C · 100% · Limited / intermittent contact
Manufacturer Ref · Ref chart ↗
Limited resistance to methyl ethyl ketone (MEK) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PVDF unsuitable for continuous pressurized containment.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to methyl ethyl ketone (MEK) at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to methyl ethyl ketone (MEK) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to methyl ethyl ketone (MEK) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to Methyl Ethyl Ketone (MEK) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to Methyl Ethyl Ketone (MEK) at 20 °C with negligible swelling, weight change, or mechanical degradation in EPDM rubber.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Methyl Ethyl Ketone (MEK) causes rapid swelling, softening, and seal failure in FKM (Viton) fluoroelastomer; consider EPDM or PTFE/FEP-encapsulated seals instead.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Methyl Ethyl Ketone (MEK) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: Methyl Ethyl Ketone (MEK) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Dehydrogenation of sec-butanol derived from n-butenes
  • Liquid-phase oxidation of n-butane
Downstream Derivatives
  • Methyl ethyl ketone peroxide (MEKP) initiator for unsaturated polyesters
  • Solvent-based polyurethane and PVC adhesives
Typical Industrial Uses
  • Solvent for vinyl coatings, acrylics, and solvent-cement welding of PVC/ABS
  • Lube oil dewaxing and magnetic tape/ink manufacturing
  • Intermediate for MEKP fiberglass resin curing catalysts

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source Methyl Ethyl Ketone (MEK) & Compatible Equipment

Methyl Ethyl Ketone Industrial / Reagent Grade (CAS 78-93-3)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Solvent-Resistant Chemical Drums, Pumps & Seals

HDPE / PTFE / FKM / EPDM solvent transfer equipment

View Suppliers on Made-in-China.com