Trichloroethylene (TCE)
Dense, non-flammable chlorinated alkene solvent used as a fluorocarbon refrigerant intermediate and in closed-loop precision metal vapor degreasing.
Also known as: Trichloroethene, Triclene, TCE
Registry Numbers & Structural Strings
| Identifier | Value |
|---|---|
| CAS Registry Number | 79-01-6 |
| EC Number | 201-167-4 |
| Molecular Formula | C2HCl3 |
| Molecular Weight | 131.38 g/mol |
| IUPAC Name | 1,1,2-trichloroethene |
| Canonical SMILES | C(=C(Cl)Cl)Cl |
| InChI | InChI=1S/C2HCl3/c3-1-2(4)5/h1H |
| InChIKey | XSTXAVWGXDQKEL-UHFFFAOYSA-N |
| UN Transport Number | UN1710 |
| PubChem CID | 6575 |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 6575
Measured Constants (SI / Imperial)
Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous Trichloroethylene (TCE) (CAS 79-01-6) unless otherwise noted.
| Property | Value |
|---|---|
| Physical State | Liquid |
| Appearance | Dense, colorless non-flammable liquid with sweet chloroform-like odor |
| Density | 1.464 g/cm³ (20 °C) (12.22 lb/gal) |
| Melting Point | -84.8 °C (-120.6 °F) |
| Boiling Point | 87.2 °C (189 °F) |
| Flash Point | — |
| Vapor Pressure | 69.0 mmHg (25 °C) |
| Water Solubility | 1.28 g/L (25 °C) |
| pH / pKa | Neutral chlorinated alkene |
| Viscosity | 0.545 mPa·s (25 °C) |
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
GHS Classification & Precautions
- H315+H319: Causes skin and serious eye irritation
- H336: May cause drowsiness or dizziness
- H341: Suspected of causing genetic defects
- H350: May cause cancer
- P201: Obtain special instructions before use
- P261: Avoid breathing vapors
- P280: Use closed vapor-degreasing equipment and Viton/PVA gloves
Handling & storage: Store stabilized in dark, cool containers away from strong alkalis (forms explosive dichloroacetylene) and aluminum dust. Destroys ABS, PC, PS, PVC-U, PMMA, EPDM, NBR; use PTFE, FEP, PFA, PVDF, PEEK, PPS, or FKM.
Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25
Plastics in Contact with Trichloroethylene (TCE)
Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.
| Plastic Family | Rating & Conditions | Engineering Notes |
|---|---|---|
| Polypropylene (PP)
ISO 1043: PP | Limited resistance to Trichloroethylene (TCE) at 20 °C; moderate swelling, softening, or stress-cracking risk makes polypropylene (PP) unsuitable for continuous containment. Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C) | |
| High-Density Polyethylene (HDPE)
ISO 1043: PE-HD | Limited resistance to Trichloroethylene (TCE) at 20 °C; moderate swelling, softening, or stress-cracking risk makes HDPE unsuitable for continuous containment. Grade basis: High-density polyethylene (PE100 / blow-molding HDPE) | |
| Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in ABS even under short-term contact. Grade basis: General-purpose unreinforced ABS molding grade | |
| Polycarbonate (PC)
ISO 1043: PC | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact. Grade basis: Unfilled bisphenol-A polycarbonate (PC) | |
| Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66 | Limited resistance to Trichloroethylene (TCE) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PA66 (Nylon 66) unsuitable for continuous containment. Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66) | |
| Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in LDPE even under short-term contact. Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade) | |
| Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact. Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade) | |
| Polystyrene (GPPS) (PS)
ISO 1043: PS | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact. Grade basis: General-purpose crystal polystyrene (GPPS) | |
| Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6 | Limited resistance to Trichloroethylene (TCE) at 20 °C; moderate swelling, softening, or stress-cracking risk makes PA6 (Nylon 6) unsuitable for continuous containment. Grade basis: Unreinforced polyamide 6 (extruded/molded PA6) | |
| Polyoxymethylene (Acetal) (POM)
ISO 1043: POM | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in acetal (POM) even under short-term contact. Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H) | |
| Polybutylene Terephthalate (PBT)
ISO 1043: PBT | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in PBT even under short-term contact. Grade basis: Unreinforced polybutylene terephthalate (PBT) | |
| Polyethylene Terephthalate (PET)
ISO 1043: PET | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in PET even under short-term contact. Grade basis: Semi-crystalline / oriented PET resin | |
| Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact. Grade basis: Cast & extruded polymethyl methacrylate (PMMA) | |
| Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW | Limited resistance to Trichloroethylene (TCE) at 20 °C; moderate swelling, softening, or stress-cracking risk makes UHMWPE unsuitable for continuous containment. Grade basis: Virgin compression-molded UHMWPE (>3M g/mol) | |
| Styrene-Acrylonitrile (SAN)
ISO 1043: SAN | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in SAN even under short-term contact. Grade basis: Transparent styrene-acrylonitrile copolymer (SAN) | |
| Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE | Virtually inert to Trichloroethylene (TCE) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade) | |
| Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF | Excellent resistance to Trichloroethylene (TCE) at 20 °C with negligible swelling, weight change, or mechanical degradation in PVDF. Grade basis: Homopolymer PVDF (pipe, valve & sheet grade) | |
| Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP | Good resistance to Trichloroethylene (TCE) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature. Grade basis: Melt-extruded FEP tubing & lining grade | |
| Polyether Ether Ketone (PEEK)
ISO 1043: PEEK | Excellent resistance to Trichloroethylene (TCE) at 20 °C with negligible swelling, weight change, or mechanical degradation in PEEK. Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class) | |
| Polyphenylene Sulfide (PPS)
ISO 1043: PPS | Excellent resistance to Trichloroethylene (TCE) at 20 °C with negligible swelling, weight change, or mechanical degradation in PPS. Grade basis: Linear / 40% glass-filled PPS (PPS-GF40) | |
| Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA | Virtually inert to Trichloroethylene (TCE) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact. Grade basis: High-purity melt-processable PFA tubing & lining grade | |
| Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM | Not recommended: Trichloroethylene (TCE) severely swells and degrades EPDM rubber; specify FKM (Viton) or PTFE/PFA seals for hydrocarbon or strong-acid service. Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A) | |
| Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM | Excellent resistance to Trichloroethylene (TCE) at 20 °C with negligible swelling, weight change, or mechanical degradation in FKM (Viton) fluoroelastomer. Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine) | |
| Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact. Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N) | |
| Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ | Not recommended: Trichloroethylene (TCE) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact. Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ) |
Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25
Upstream, Downstream & Applications
- Chlorination/oxychlorination of ethylene or 1,2-dichloroethane
- HFC-134a / HFO refrigerant chemical intermediate
- Closed-loop aerospace and precision metal vapor degreasing
- Intermediate for fluorocarbon refrigerants
- Heavy-duty vapor degreasing of precision metal parts (where permitted)
- Solvent in specialty adhesives and extraction
Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25
Source Trichloroethylene (TCE) & Compatible Equipment
High-purity industrial grade · Bulk supply
View Suppliers on Made-in-China.comHDPE / PTFE / FKM / EPDM solvent transfer equipment
View Suppliers on Made-in-China.com