CHEMICAL · CAS 872-50-4

N-Methyl-2-pyrrolidone (NMP)

CAS 872-50-4 · EC 212-828-1 · C5H9NO

High-boiling cyclic amide polar aprotic solvent that is the global industry standard for dissolving PVDF binder in lithium-ion battery cathode slurries, as well as aramid fiber spinning and electronics cleaning.

Also known as: 1-Methyl-2-pyrrolidinone, NMP, M-Pyrol

Molecular Weight
99.13 g/mol
Boiling Point
202 °C
Melting Point
-24 °C
Flash Point
91 °C
Density
1.028 g/cm³
CHEMICAL IDENTIFIERS

Registry Numbers & Structural Strings

N-Methyl-2-pyrrolidone (NMP) chemical identifiers
Identifier Value
CAS Registry Number 872-50-4
EC Number 212-828-1
Molecular Formula C5H9NO
Molecular Weight 99.13 g/mol
IUPAC Name 1-methylpyrrolidin-2-one
Canonical SMILES CN1CCCC1=O
InChI InChI=1S/C5H9NO/c1-6-4-2-3-5(6)7/h2-4H2,1H3
InChIKey SECXISVLQFMRJM-UHFFFAOYSA-N
UN Transport Number —
PubChem CID 13387

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25 · CID 13387

PHYSICAL & CHEMICAL PROPERTIES

Measured Constants (SI / Imperial)

Neat / Pure Substance Basis MEASUREMENT BASIS

Identifiers, physical constants, and 20 °C compatibility ratings refer to neat / anhydrous N-Methyl-2-pyrrolidone (NMP) (CAS 872-50-4) unless otherwise noted.

Density (vs. Water = 1.0)1.028 g/cm³
0.5Water 1.02.5
Melting / Freezing Point-24 °C
-13020 °C260
Boiling Point202 °C
-50Water 100 °C350
Flash Point (Closed Cup)91 °C
-50GHS Cat.2 (23 °C)220
N-Methyl-2-pyrrolidone (NMP) physical and chemical properties
Property Value
Physical State Liquid
Appearance Colorless to pale yellow high-boiling liquid with mild amine odor
Density 1.028 g/cm³ (25 °C) (8.58 lb/gal)
Melting Point -24 °C (-11.2 °F)
Boiling Point 202 °C (395.6 °F)
Flash Point 91 °C (195.8 °F (closed cup))
Vapor Pressure 0.34 mmHg (25 °C)
Water Solubility Miscible in all proportions
pH / pKa pH 7.7 – 8.0 (10% aqueous)
Viscosity 1.65 mPa·s (25 °C)

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SAFETY & HANDLING

GHS Classification & Precautions

GHS SAFETY & HAZARD CLASSIFICATION Signal word: Danger
GHS08 Health Hazard
GHS07 Irritant / Harmful
Reproductive Toxicity (Category 1B) · Skin Irritation (Category 2) · Serious Eye Irritation (Category 2A) · STOT — Single Exposure (Category 3, respiratory)
Hazard statements
  • H315: Causes skin irritation
  • H319: Causes serious eye irritation
  • H335: May cause respiratory irritation
  • H360D: May damage the unborn child
Key precautionary statements
  • P201: Obtain special instructions before use
  • P280: Wear butyl-rubber gloves and eye protection
  • P261: Avoid breathing vapors or mist

Handling & storage: Store in tightly closed containers away from strong acids and oxidizers. Actively dissolves PVDF, ABS, PC, PVC-U, PS, PMMA, and SAN; use PTFE, FEP, PEEK, PPS, or stainless steel in battery slurry lines.

Source: PubChem (NIH) / ECHA / NOAA CAMEO (GHS Classification Summary) · Retrieved 2026-11-25

COMPATIBILITY MODULE

Plastics in Contact with N-Methyl-2-pyrrolidone (NMP)

View full matrix →

Compatibility grades indicate expected chemical resistance of unreinforced polymer families under stated test conditions. Always verify stressed parts and elevated temperatures via immersion testing.

Plastic compatibility with N-Methyl-2-pyrrolidone (NMP)
Plastic Family Rating & Conditions Engineering Notes
Polypropylene (PP)
ISO 1043: PP
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to N-methyl-2-pyrrolidone (NMP) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced PP homopolymer (PP-H) & copolymer (PP-C)
High-Density Polyethylene (HDPE)
ISO 1043: PE-HD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to N-methyl-2-pyrrolidone (NMP) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: High-density polyethylene (PE100 / blow-molding HDPE)
Acrylonitrile Butadiene Styrene (ABS)
ISO 1043: ABS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N-methyl-2-pyrrolidone (NMP) causes severe chemical attack, dissolution, crazing, or rapid structural failure in ABS even under short-term contact.
Grade basis: General-purpose unreinforced ABS molding grade
Polycarbonate (PC)
ISO 1043: PC
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N-methyl-2-pyrrolidone (NMP) causes severe chemical attack, dissolution, crazing, or rapid structural failure in polycarbonate (PC) even under short-term contact.
Grade basis: Unfilled bisphenol-A polycarbonate (PC)
Polyamide 66 (Nylon 66) (PA66)
ISO 1043: PA66
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to N-methyl-2-pyrrolidone (NMP) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA66 (Nylon 66).
Grade basis: Unreinforced polyamide 66 (dry-as-molded / conditioned PA66)
Low-Density Polyethylene (LDPE)
ISO 1043: PE-LD
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to N-methyl-2-pyrrolidone (NMP) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Unfilled low-density polyethylene (LDPE film/bottle grade)
Unplasticized Polyvinyl Chloride (Rigid PVC) (PVC-U)
ISO 1043: PVC-U
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N-methyl-2-pyrrolidone (NMP) causes severe chemical attack, dissolution, crazing, or rapid structural failure in rigid PVC (PVC-U) even under short-term contact.
Grade basis: Rigid unplasticized PVC (Schedule 40/80 pipe & sheet grade)
Polystyrene (GPPS) (PS)
ISO 1043: PS
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N-methyl-2-pyrrolidone (NMP) causes severe chemical attack, dissolution, crazing, or rapid structural failure in polystyrene (PS) even under short-term contact.
Grade basis: General-purpose crystal polystyrene (GPPS)
Polyamide 6 (Nylon 6) (PA6)
ISO 1043: PA6
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to N-methyl-2-pyrrolidone (NMP) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PA6 (Nylon 6).
Grade basis: Unreinforced polyamide 6 (extruded/molded PA6)
Polyoxymethylene (Acetal) (POM)
ISO 1043: POM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to N-methyl-2-pyrrolidone (NMP) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Acetal copolymer (POM-C) & homopolymer (POM-H)
Polybutylene Terephthalate (PBT)
ISO 1043: PBT
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to N-methyl-2-pyrrolidone (NMP) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Unreinforced polybutylene terephthalate (PBT)
Polyethylene Terephthalate (PET)
ISO 1043: PET
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to N-methyl-2-pyrrolidone (NMP) at 20 °C; minor absorption, slight swelling, or gradual property change possible over prolonged exposure or elevated temperature.
Grade basis: Semi-crystalline / oriented PET resin
Polymethyl Methacrylate (Acrylic) (PMMA)
ISO 1043: PMMA
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N-methyl-2-pyrrolidone (NMP) causes severe chemical attack, dissolution, crazing, or rapid structural failure in acrylic (PMMA) even under short-term contact.
Grade basis: Cast & extruded polymethyl methacrylate (PMMA)
Ultra-High-Molecular-Weight Polyethylene (UHMWPE)
ISO 1043: PE-UHMW
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to N-methyl-2-pyrrolidone (NMP) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed UHMWPE.
Grade basis: Virgin compression-molded UHMWPE (>3M g/mol)
Styrene-Acrylonitrile (SAN)
ISO 1043: SAN
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N-methyl-2-pyrrolidone (NMP) causes severe chemical attack, dissolution, crazing, or rapid structural failure in SAN even under short-term contact.
Grade basis: Transparent styrene-acrylonitrile copolymer (SAN)
Polytetrafluoroethylene (PTFE)
ISO 1043: PTFE
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to N-methyl-2-pyrrolidone (NMP) at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Virgin sintered PTFE (sheet, liner & gasket grade)
Polyvinylidene Fluoride (PVDF)
ISO 1043: PVDF
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Severe attack: N-methyl-2-pyrrolidone (NMP) is an active polar aprotic solvent that rapidly swells and dissolves PVDF. Specify PTFE, FEP, PEEK, or PPS instead.
Grade basis: Homopolymer PVDF (pipe, valve & sheet grade)
Fluorinated Ethylene Propylene (FEP)
ISO 1043: FEP
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to N-methyl-2-pyrrolidone (NMP) at 20 °C and elevated service temperatures; standard fluoropolymer lining and seal choice for aggressive media.
Grade basis: Melt-extruded FEP tubing & lining grade
Polyether Ether Ketone (PEEK)
ISO 1043: PEEK
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to N-methyl-2-pyrrolidone (NMP) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PEEK.
Grade basis: Unfilled semi-crystalline PEEK (Victrex/KetaSpire class)
Polyphenylene Sulfide (PPS)
ISO 1043: PPS
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Excellent resistance to N-methyl-2-pyrrolidone (NMP) at 20 °C with negligible swelling, weight change, or mechanical loss in unstressed PPS.
Grade basis: Linear / 40% glass-filled PPS (PPS-GF40)
Perfluoroalkoxy Alkane (PFA)
ISO 1043: PFA
A Excellent 20 °C · 100% · Continuous immersion
Manufacturer Ref · Ref chart ↗
Virtually inert to N-Methyl-2-pyrrolidone (NMP) at 20 °C and elevated service temperatures; standard perfluoropolymer choice for corrosive process contact.
Grade basis: High-purity melt-processable PFA tubing & lining grade
Ethylene Propylene Diene Monomer (EPDM)
ISO 1629: EPDM
B Good 20 °C · 100% · Ambient contact
Manufacturer Ref · Ref chart ↗
Good resistance to N-Methyl-2-pyrrolidone (NMP) at 20 °C; minor absorption or slight property shift possible over prolonged exposure or elevated temperature.
Grade basis: Peroxide-cured EPDM elastomer (70–80 Shore A)
Fluoroelastomer (Viton) (FKM)
ISO 1629: FKM
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N-Methyl-2-pyrrolidone (NMP) causes rapid swelling, softening, and seal failure in FKM (Viton) fluoroelastomer; consider EPDM or PTFE/FEP-encapsulated seals instead.
Grade basis: Standard Type A FKM fluoroelastomer (66% fluorine)
Nitrile Butadiene Rubber (Buna-N) (NBR)
ISO 1629: NBR
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N-Methyl-2-pyrrolidone (NMP) causes severe attack, swelling, crazing, or rapid structural failure in NBR (Buna-N) nitrile rubber even under short-term contact.
Grade basis: Medium-to-high ACN nitrile rubber (NBR / Buna-N)
Silicone Rubber (VMQ) (VMQ)
ISO 1629: VMQ
D Not recommended 20 °C · 100% · Short-term contact
Manufacturer Ref · Ref chart ↗
Not recommended: N-Methyl-2-pyrrolidone (NMP) causes severe attack, swelling, crazing, or rapid structural failure in VMQ silicone rubber even under short-term contact.
Grade basis: Platinum- or peroxide-cured methyl vinyl silicone (VMQ)

Source: Cole-Parmer / Thermo Scientific (Nalgene) / GF Piping Consensus · Retrieved 2026-11-25

INDUSTRIAL CONTEXT

Upstream, Downstream & Applications

Upstream Feedstocks
  • Condensation of gamma-butyrolactone (GBL) with methylamine
Downstream Derivatives
  • Lithium-ion battery cathode slurry (PVDF + NMP) manufacturing
  • Polyimide and polyamide-imide wire enamels
  • Petrochemical butadiene and BTX extractive distillation
Typical Industrial Uses
  • Primary solvent for PVDF binder in EV lithium-ion battery electrode coating
  • Semiconductor photoresist stripping and precision cleaning
  • Solvent for high-temperature PPS, aramid, and polyimide polymerization

Source: PubChem (NIH) / ECHA / NOAA CAMEO · Retrieved 2026-11-25

SPECIFICATION-MATCHED SOURCING

Source N-Methyl-2-pyrrolidone (NMP) & Compatible Equipment

N-Methyl-2-pyrrolidone Industrial / Reagent Grade (CAS 872-50-4)

High-purity industrial grade · Bulk supply

View Suppliers on Made-in-China.com
Solvent-Resistant Chemical Drums, Pumps & Seals

HDPE / PTFE / FKM / EPDM solvent transfer equipment

View Suppliers on Made-in-China.com